Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.376 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 253.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 284.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 189.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 197.0 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 197.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 84.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 278.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 58.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 84.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 253.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 190.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 227.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 112.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 227.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 140.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 177.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 281.4 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 317.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 168.8 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 170.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 177.0 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 317.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 152.8 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 177.0 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 126.4 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 281.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 264.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 113.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 278.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 284.4 |
Ag (mp-124) | <1 1 0> | <1 1 1> | 190.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 227.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 25.3 |
GaSe (mp-1943) | <1 0 1> | <1 1 0> | 264.8 |
BN (mp-984) | <1 1 0> | <1 0 0> | 168.8 |
BN (mp-984) | <1 1 1> | <1 0 1> | 232.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 151.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 113.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 190.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 253.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 168.8 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 0 0> | 253.3 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 337.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 168.8 |
MoS2 (mp-1434) | <1 0 0> | <1 1 0> | 264.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 253.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 190.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 227.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 227.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 113.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbMg6Zr (mp-1022517) | 0.5327 | 0.271 | 3 |
LuAl2Pd5 (mp-1025564) | 0.5280 | 0.000 | 3 |
ZnCdPt2 (mp-30493) | 0.5120 | 0.000 | 3 |
KMg6Ti (mp-1021423) | 0.5174 | 0.255 | 3 |
BaMg6Nb (mp-1016650) | 0.5329 | 0.270 | 3 |
In3Pd5 (mp-22146) | 0.3492 | 0.000 | 2 |
ZrGa2 (mp-30683) | 0.4637 | 0.000 | 2 |
Mn3Pd5 (mp-1078895) | 0.1807 | 0.000 | 2 |
VIr (mp-1079131) | 0.1397 | 0.019 | 2 |
Al3Ni5 (mp-16514) | 0.2212 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ga_d Ni_pv |
Final Energy/Atom-5.1238 eV |
Corrected Energy-40.9902 eV
Uncorrected energy = -40.9902 eV
Corrected energy = -40.9902 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)