Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.169 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 256.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 142.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 256.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 1> | 256.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 268.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 161.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 132.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 335.9 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 146.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 235.2 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 190.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 168.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 264.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 132.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 235.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 235.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 132.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 335.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 190.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 168.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 337.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 237.5 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 293.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 44.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 146.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 220.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 142.5 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 149.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 132.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 235.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 235.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 256.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 302.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 190.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 323.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 47.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 264.2 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 285.1 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 293.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 249.6 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 198.9 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 256.6 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 183.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 95.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 298.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 256.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 110.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
196 | 65 | 46 | 0 | 0 | 0 |
65 | 196 | 46 | 0 | 0 | 0 |
46 | 46 | 251 | 0 | 0 | 0 |
0 | 0 | 0 | 69 | 0 | 0 |
0 | 0 | 0 | 0 | 69 | 0 |
0 | 0 | 0 | 0 | 0 | 108 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.9 | -1.8 | -0.7 | 0 | 0 | 0 |
-1.8 | 5.9 | -0.7 | 0 | 0 | 0 |
-0.7 | -0.7 | 4.2 | 0 | 0 | 0 |
0 | 0 | 0 | 14.5 | 0 | 0 |
0 | 0 | 0 | 0 | 14.5 | 0 |
0 | 0 | 0 | 0 | 0 | 9.3 |
Shear Modulus GV82 GPa |
Bulk Modulus KV106 GPa |
Shear Modulus GR78 GPa |
Bulk Modulus KR106 GPa |
Shear Modulus GVRH80 GPa |
Bulk Modulus KVRH106 GPa |
Elastic Anisotropy0.22 |
Poisson's Ratio0.20 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaCo2Ni (mp-20551) | 0.5713 | 0.080 | 3 |
MnGaFe2 (mp-1065753) | 0.5991 | 0.053 | 3 |
HfTl3 (mp-982930) | 0.0486 | 0.260 | 2 |
NpPa3 (mp-973994) | 0.0458 | 0.299 | 2 |
NbGa3 (mp-1973) | 0.0452 | 0.000 | 2 |
ZrAl3 (mp-1065309) | 0.0446 | 0.025 | 2 |
U3Cl (mp-972405) | 0.0325 | 0.820 | 2 |
Rb (mp-975519) | 0.5556 | 0.017 | 1 |
Ba (mp-1058581) | 0.5059 | 0.019 | 1 |
Cs (mp-1012110) | 0.5778 | 0.046 | 1 |
Ga (mp-140) | 0.5528 | 0.029 | 1 |
In (mp-1055994) | 0.5332 | 0.030 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Ga_d |
Final Energy/Atom-5.4046 eV |
Corrected Energy-21.6183 eV
-21.6183 eV = -21.6183 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)