material

HfPt3

ID:

mp-11456

DOI:

10.17188/1187848


Tags: Hafnium platinum (1/3) Platinum hafnium (3/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.090 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
19.26 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 104258 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.005 197.4
Al (mp-134) <1 1 1> <0 0 1> 0.005 28.2
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.007 28.2
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.009 197.4
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.009 276.5
C (mp-48) <0 0 1> <0 0 1> 0.013 84.6
BN (mp-984) <0 0 1> <0 0 1> 0.014 197.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.016 28.2
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.030 338.4
InAs (mp-20305) <1 1 1> <0 0 1> 0.046 197.4
ZnO (mp-2133) <1 1 0> <1 0 0> 0.046 212.8
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.065 197.4
GaSe (mp-1943) <0 0 1> <0 0 1> 0.068 112.8
Ni (mp-23) <1 0 0> <0 0 1> 0.071 197.4
TePb (mp-19717) <1 1 0> <1 1 0> 0.078 184.3
Ni (mp-23) <1 1 1> <0 0 1> 0.084 84.6
CaF2 (mp-2741) <1 1 0> <1 0 1> 0.094 301.1
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.099 184.3
GaP (mp-2490) <1 1 0> <1 0 1> 0.104 301.1
CdS (mp-672) <0 0 1> <0 0 1> 0.117 197.4
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.153 120.4
KP(HO2)2 (mp-23959) <0 0 1> <1 0 1> 0.156 301.1
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.167 289.1
MoSe2 (mp-1634) <1 1 0> <1 0 0> 0.172 266.0
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.173 180.6
NdGaO3 (mp-3196) <0 1 0> <1 0 1> 0.178 301.1
CdTe (mp-406) <1 1 0> <1 1 0> 0.187 184.3
Mg (mp-153) <0 0 1> <0 0 1> 0.190 112.8
GaN (mp-804) <0 0 1> <0 0 1> 0.195 253.8
Ag (mp-124) <1 0 0> <0 0 1> 0.212 310.2
GaN (mp-804) <1 0 0> <1 1 1> 0.221 289.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.221 253.8
InSb (mp-20012) <1 1 0> <1 1 0> 0.231 184.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.242 253.8
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.248 159.6
TeO2 (mp-2125) <1 0 0> <1 0 0> 0.253 212.8
Au (mp-81) <1 1 1> <0 0 1> 0.262 366.6
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.271 159.6
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.286 319.2
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.291 266.0
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.302 319.2
InSb (mp-20012) <1 0 0> <1 0 0> 0.318 266.0
Au (mp-81) <1 0 0> <0 0 1> 0.318 310.2
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.343 276.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.345 266.0
CdSe (mp-2691) <1 1 1> <0 0 1> 0.359 197.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.360 112.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.362 112.8
Cu (mp-30) <1 1 0> <0 0 1> 0.364 366.6
AlN (mp-661) <1 1 1> <1 1 1> 0.365 289.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
388 163 149 0 0 0
163 388 149 0 0 0
149 149 398 0 0 0
0 0 0 91 0 0
0 0 0 0 91 0
0 0 0 0 0 113
Compliance Tensor Sij (10-12Pa-1)
3.4 -1.1 -0.9 0 0 0
-1.1 3.4 -0.9 0 0 0
-0.9 -0.9 3.2 0 0 0
0 0 0 10.9 0 0
0 0 0 0 10.9 0
0 0 0 0 0 8.9
Shear Modulus GV
107 GPa
Bulk Modulus KV
233 GPa
Shear Modulus GR
105 GPa
Bulk Modulus KR
233 GPa
Shear Modulus GVRH
106 GPa
Bulk Modulus KVRH
233 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.1954 0.028 4
CrFeCoNi (mp-1012640) 0.2505 0.065 4
CrFeCoNi (mp-1096923) 0.3303 0.193 4
Mg13Au41 (mp-30407) 0.0771 0.023 2
MgAu3 (mp-30408) 0.0774 0.000 2
BiPd3 (mp-30463) 0.0688 0.000 2
HfPd3 (mp-11453) 0.0205 0.000 2
ZrPd3 (mp-30842) 0.0180 0.000 2
Sm (mp-69) 0.0661 0.000 1
Mg (mp-973364) 0.0665 0.013 1
Pr (mp-38) 0.0662 0.000 1
Pm (mp-867200) 0.0661 0.000 1
Nd (mp-123) 0.0661 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Pt
Final Energy/Atom
-8.1321 eV
Corrected Energy
-130.1138 eV
Uncorrected energy = -130.1138 eV Corrected energy = -130.1138 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104258
  • 638782
Submitted by
User remarks:
  • Hafnium platinum (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)