material

Hg2Pt

ID:

mp-11470

DOI:

10.17188/1187862


Tags: Mercury platinum (2/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.058 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.021 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.14 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Hg4Pt + Pt
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 104339 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 1 0> <1 0 1> 0.003 137.6
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.004 137.6
Cu (mp-30) <1 0 0> <0 0 1> 0.016 117.1
SiC (mp-8062) <1 1 1> <1 1 0> 0.021 265.9
Al (mp-134) <1 1 0> <1 0 1> 0.023 137.6
LiTaO3 (mp-3666) <0 0 1> <1 1 0> 0.024 163.7
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.024 210.8
C (mp-48) <0 0 1> <1 1 0> 0.024 163.7
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.037 231.4
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.043 210.8
TiO2 (mp-390) <1 0 0> <1 0 1> 0.045 110.1
C (mp-48) <1 0 1> <1 0 0> 0.054 159.1
LiGaO2 (mp-5854) <1 0 0> <1 1 1> 0.055 248.8
C (mp-48) <1 1 1> <1 0 0> 0.059 101.3
TiO2 (mp-390) <0 0 1> <0 0 1> 0.064 117.1
GaTe (mp-542812) <1 0 0> <1 1 0> 0.068 225.0
ZrO2 (mp-2858) <1 0 -1> <1 1 0> 0.070 143.2
LiNbO3 (mp-3731) <0 0 1> <1 1 0> 0.073 163.7
Fe2O3 (mp-24972) <1 1 0> <1 1 0> 0.079 122.7
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.085 159.1
ZrO2 (mp-2858) <1 1 1> <1 1 0> 0.091 102.3
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.093 281.0
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.096 159.1
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.100 55.1
GaN (mp-804) <1 0 1> <1 0 0> 0.102 57.9
AlN (mp-661) <1 1 0> <1 1 0> 0.121 81.8
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.123 351.3
DyScO3 (mp-31120) <1 0 0> <1 0 1> 0.129 137.6
InP (mp-20351) <1 1 1> <1 0 1> 0.133 247.7
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.134 351.3
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.134 231.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.138 286.4
PbS (mp-21276) <1 1 1> <1 0 1> 0.143 247.7
Ge (mp-32) <1 0 0> <1 0 1> 0.156 165.2
Cu (mp-30) <1 1 0> <1 0 0> 0.159 130.2
CdS (mp-672) <0 0 1> <1 0 1> 0.161 247.7
TbScO3 (mp-31119) <1 0 0> <1 0 1> 0.162 137.6
Au (mp-81) <1 1 1> <1 0 0> 0.162 274.8
CdS (mp-672) <1 1 1> <0 0 1> 0.168 210.8
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.170 231.4
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.172 137.6
Te2W (mp-22693) <0 1 1> <0 0 1> 0.176 117.1
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.179 217.7
Te2W (mp-22693) <1 0 0> <1 0 0> 0.180 289.3
TbScO3 (mp-31119) <1 0 1> <1 0 1> 0.180 55.1
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.187 163.7
SiC (mp-7631) <1 0 0> <1 0 0> 0.191 231.4
C (mp-66) <1 0 0> <0 0 1> 0.193 117.1
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.199 40.9
Au (mp-81) <1 1 0> <1 1 0> 0.202 122.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
183 66 66 0 0 0
66 131 34 0 0 0
66 34 131 0 0 0
0 0 0 11 0 0
0 0 0 0 24 0
0 0 0 0 0 24
Compliance Tensor Sij (10-12Pa-1)
7.7 -3.1 -3.1 0 0 0
-3.1 9.4 -0.9 0 0 0
-3.1 -0.9 9.4 0 0 0
0 0 0 93.3 0 0
0 0 0 0 41.5 0
0 0 0 0 0 41.5
Shear Modulus GV
30 GPa
Bulk Modulus KV
86 GPa
Shear Modulus GR
23 GPa
Bulk Modulus KR
81 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
83 GPa
Elastic Anisotropy
1.79
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Hg2Rh (mp-11870) 0.5417 0.004 2
ZrSn (mp-1094528) 0.7118 0.174 2
Cu (mp-1059259) 0.7284 0.143 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hg Pt
Final Energy/Atom
-2.2840 eV
Corrected Energy
-6.8519 eV
Uncorrected energy = -6.8519 eV Corrected energy = -6.8519 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 104339
Submitted by
User remarks:
  • Mercury platinum (2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)