Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.306 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi15Pd4 + Li2Pd |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
InAs (mp-20305) | <1 0 0> | <1 0 0> | 0.000 | 38.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 0.000 | 54.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 0.000 | 66.2 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 0.000 | 38.2 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 0.000 | 54.1 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 0.000 | 66.2 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 0.000 | 191.1 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 0.001 | 66.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 0.001 | 344.0 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 0.001 | 305.8 |
C (mp-66) | <1 1 0> | <1 1 0> | 0.002 | 54.1 |
C (mp-66) | <1 1 1> | <1 1 1> | 0.002 | 66.2 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 0.002 | 198.6 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 0.002 | 38.2 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 0.002 | 191.1 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 0.003 | 54.1 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 0.003 | 162.2 |
Al (mp-134) | <1 1 1> | <1 1 1> | 0.004 | 198.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 0.004 | 198.6 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 0.004 | 152.9 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 0.006 | 305.8 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 0.009 | 267.6 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.009 | 305.8 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 0.012 | 267.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 0.013 | 152.9 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 0.013 | 264.8 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 0.014 | 267.6 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 0.014 | 305.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 0.015 | 198.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 0.015 | 162.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 0.016 | 198.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 0.017 | 38.2 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 0.017 | 305.8 |
WSe2 (mp-1821) | <0 0 1> | <1 1 0> | 0.018 | 270.3 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 0.018 | 270.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 0.018 | 191.1 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 0.019 | 66.2 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 0.020 | 54.1 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 0.021 | 66.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 0.022 | 344.0 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 0.022 | 344.0 |
C (mp-66) | <1 0 0> | <1 1 0> | 0.022 | 270.3 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 0.022 | 191.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 0.022 | 324.4 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 0.023 | 152.9 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 0.024 | 38.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 0.024 | 305.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 0.024 | 152.9 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 0.025 | 305.8 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 0.025 | 229.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
39 | 36 | 36 | 0 | 0 | 0 |
36 | 39 | 36 | 0 | 0 | 0 |
36 | 36 | 39 | 0 | 0 | 0 |
0 | 0 | 0 | 30 | 0 | 0 |
0 | 0 | 0 | 0 | 30 | 0 |
0 | 0 | 0 | 0 | 0 | 30 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
183.9 | -87.4 | -87.4 | 0 | 0 | 0 |
-87.4 | 183.9 | -87.4 | 0 | 0 | 0 |
-87.4 | -87.4 | 183.9 | 0 | 0 | 0 |
0 | 0 | 0 | 33.3 | 0 | 0 |
0 | 0 | 0 | 0 | 33.3 | 0 |
0 | 0 | 0 | 0 | 0 | 33.3 |
Shear Modulus GV19 GPa |
Bulk Modulus KV37 GPa |
Shear Modulus GR4 GPa |
Bulk Modulus KR37 GPa |
Shear Modulus GVRH11 GPa |
Bulk Modulus KVRH37 GPa |
Elastic Anisotropy17.22 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VCo2Sn (mp-21469) | 0.0000 | 0.054 | 3 |
Li2GaAu (mp-30381) | 0.0000 | 0.000 | 3 |
CeMgZn2 (mp-13254) | 0.0000 | 0.000 | 3 |
MnAlPt2 (mp-10893) | 0.0000 | 0.448 | 3 |
ScSnPt2 (mp-30844) | 0.0000 | 0.052 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.088 | 4 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.096 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
SmMg3 (mp-30779) | 0.0000 | 0.065 | 2 |
Ni3Sb (mp-10260) | 0.0000 | 0.044 | 2 |
Li3Au (mp-11247) | 0.0000 | 0.000 | 2 |
LaF3 (mp-13181) | 0.0000 | 0.181 | 2 |
Cu3Sb (mp-2002) | 0.0000 | 0.181 | 2 |
Se (mp-119) | 0.0000 | 0.602 | 1 |
Er (mp-10753) | 0.0000 | 0.143 | 1 |
Nd (mp-4) | 0.0000 | 0.140 | 1 |
Tm (mp-10661) | 0.0000 | 0.140 | 1 |
Pb (mp-22692) | 0.0000 | 0.048 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Pd |
Final Energy/Atom-3.0321 eV |
Corrected Energy-12.1284 eV
-12.1284 eV = -12.1284 eV (uncorrected energy)
|