Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.143 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLuPb3 + Lu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 279.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 161.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 161.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 143.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 329.2 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 197.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 128.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 264.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 44.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 220.3 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 192.5 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 329.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 190.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 192.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 317.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 132.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 192.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 190.9 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 238.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 256.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 128.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 192.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 220.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 279.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 323.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 132.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 132.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 64.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 263.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 132.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 317.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 293.7 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 329.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 249.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 264.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 293.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 337.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 132.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 192.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 279.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 235.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 249.6 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 323.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 308.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 73.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 192.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 367.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
41 | 57 | 47 | 0 | 0 | 0 |
57 | 41 | 47 | 0 | 0 | 0 |
47 | 47 | 57 | 0 | 0 | 0 |
0 | 0 | 0 | 26 | 0 | 0 |
0 | 0 | 0 | 0 | 26 | 0 |
0 | 0 | 0 | 0 | 0 | 5 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-8.3 | 53.6 | -37.2 | 0 | 0 | 0 |
53.6 | -8.3 | -37.2 | 0 | 0 | 0 |
-37.2 | -37.2 | 78.8 | 0 | 0 | 0 |
0 | 0 | 0 | 38.4 | 0 | 0 |
0 | 0 | 0 | 0 | 38.4 | 0 |
0 | 0 | 0 | 0 | 0 | 191.4 |
Shear Modulus GV11 GPa |
Bulk Modulus KV49 GPa |
Shear Modulus GR13 GPa |
Bulk Modulus KR49 GPa |
Shear Modulus GVRH12 GPa |
Bulk Modulus KVRH49 GPa |
Elastic Anisotropy-0.94 |
Poisson's Ratio0.39 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaLi5N2 (mp-29929) | 0.3152 | 0.247 | 3 |
Li3Si3Ag2 (mp-29165) | 0.3477 | 0.147 | 3 |
NaY2In (mp-635327) | 0.3663 | 0.496 | 3 |
EuAg2Sn (mp-865192) | 0.3674 | 0.016 | 3 |
GdCdPd2 (mp-866034) | 0.3730 | 1.289 | 3 |
VFeCoGe (mp-1063914) | 0.4202 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.4202 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.4202 | 0.028 | 4 |
MnFeCoGe (mp-1018024) | 0.4202 | 0.344 | 4 |
VFeCoAs (mp-1066006) | 0.4202 | 0.211 | 4 |
CaZn (mp-1038828) | 0.3168 | 0.006 | 2 |
MnFe3 (mp-999542) | 0.3136 | 0.051 | 2 |
TiMo3 (mp-1017983) | 0.3240 | 0.000 | 2 |
LiMg2 (mp-865939) | 0.3162 | 0.006 | 2 |
Mn2Au (mp-991385) | 0.2812 | 0.235 | 2 |
Be (mp-20) | 0.3513 | 0.096 | 1 |
Cs (mp-1) | 0.3554 | 0.039 | 1 |
Hg (mp-1017981) | 0.4063 | 0.001 | 1 |
S (mp-1063988) | 0.4082 | 1.137 | 1 |
Sb (mp-7761) | 0.3554 | 0.239 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Pb_d |
Final Energy/Atom-4.1248 eV |
Corrected Energy-12.3744 eV
-12.3744 eV = -12.3744 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)