material

Ni3Mo

ID:

mp-11506

DOI:

10.17188/1188016


Tags: Nickel molybdenum (3/1) Molybdenum nickel (1/3)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.093 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.51 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmmn [59]
Hall
P 2 2ab 1ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 105046 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.001 58.7
BN (mp-984) <1 0 0> <1 1 0> 0.010 154.7
InP (mp-20351) <1 1 0> <0 0 1> 0.028 151.0
Si (mp-149) <1 1 0> <0 0 1> 0.035 169.8
NdGaO3 (mp-3196) <1 0 1> <1 0 1> 0.037 322.6
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.038 169.8
GaSe (mp-1943) <1 1 0> <1 0 1> 0.039 117.3
Mg (mp-153) <1 1 1> <1 1 1> 0.042 181.2
C (mp-66) <1 1 0> <1 0 0> 0.042 89.8
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.050 169.8
WS2 (mp-224) <1 1 0> <0 1 1> 0.054 313.1
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.055 132.1
SiC (mp-11714) <1 1 0> <1 0 0> 0.065 269.4
TiO2 (mp-390) <1 1 1> <1 0 0> 0.072 269.4
GaN (mp-804) <1 0 0> <0 0 1> 0.074 169.8
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.074 216.6
InAs (mp-20305) <1 1 0> <1 1 0> 0.079 216.6
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.084 185.7
Cu (mp-30) <1 1 1> <0 0 1> 0.090 113.2
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.091 92.8
MgO (mp-1265) <1 1 1> <0 1 1> 0.093 284.6
SiC (mp-11714) <0 0 1> <1 0 1> 0.095 205.3
BaTiO3 (mp-5986) <1 0 0> <0 1 0> 0.104 85.2
InSb (mp-20012) <1 0 0> <1 0 1> 0.106 88.0
SiC (mp-7631) <0 0 1> <1 0 1> 0.106 205.3
MgF2 (mp-1249) <0 0 1> <1 0 1> 0.106 88.0
Mg (mp-153) <1 1 0> <1 1 1> 0.107 145.0
CdTe (mp-406) <1 0 0> <1 0 1> 0.108 88.0
LiNbO3 (mp-3731) <1 1 0> <1 1 1> 0.109 253.7
GaP (mp-2490) <1 1 0> <0 0 1> 0.115 169.8
TeO2 (mp-2125) <0 1 1> <0 1 1> 0.119 227.7
CdWO4 (mp-19387) <1 1 1> <1 0 1> 0.119 205.3
CdSe (mp-2691) <1 1 0> <1 1 0> 0.120 216.6
LaAlO3 (mp-2920) <0 0 1> <0 1 1> 0.131 256.1
LaAlO3 (mp-2920) <1 0 0> <1 1 0> 0.134 216.6
PbS (mp-21276) <1 1 1> <0 0 1> 0.142 188.7
SiC (mp-7631) <1 0 0> <1 1 0> 0.144 92.8
C (mp-48) <1 1 0> <0 0 1> 0.146 132.1
GaN (mp-804) <1 1 0> <0 0 1> 0.148 264.2
LiTaO3 (mp-3666) <1 1 0> <1 1 1> 0.148 253.7
BaTiO3 (mp-5986) <1 1 1> <0 1 0> 0.150 85.2
Ga2O3 (mp-886) <1 0 -1> <1 1 0> 0.150 154.7
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.152 185.7
GaSb (mp-1156) <1 1 0> <1 1 0> 0.152 216.6
ZnO (mp-2133) <1 1 1> <1 0 0> 0.157 157.1
InP (mp-20351) <1 0 0> <1 0 1> 0.159 176.0
NdGaO3 (mp-3196) <1 1 1> <0 1 0> 0.168 276.9
AlN (mp-661) <1 1 1> <1 1 0> 0.174 340.4
WS2 (mp-224) <1 0 0> <0 1 1> 0.175 313.1
BaF2 (mp-1029) <1 0 0> <1 0 1> 0.180 117.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
385 166 145 0 0 0
166 402 131 0 0 0
145 131 402 0 0 0
0 0 0 58 0 0
0 0 0 0 66 0
0 0 0 0 0 94
Compliance Tensor Sij (10-12Pa-1)
3.4 -1.1 -0.9 0 0 0
-1.1 3.1 -0.6 0 0 0
-0.9 -0.6 3 0 0 0
0 0 0 17.2 0 0
0 0 0 0 15.1 0
0 0 0 0 0 10.6
Shear Modulus GV
94 GPa
Bulk Modulus KV
230 GPa
Shear Modulus GR
85 GPa
Bulk Modulus KR
230 GPa
Shear Modulus GVRH
89 GPa
Bulk Modulus KVRH
230 GPa
Elastic Anisotropy
0.53
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.2506 0.028 4
CrFeCoNi (mp-1012640) 0.1210 0.118 4
CrFeCoNi (mp-1096923) 0.3443 0.193 4
MgCd2 (mp-1094757) 0.0866 0.032 2
Mg2Ti (mp-1094502) 0.0849 0.252 2
LiMg (mp-1094589) 0.0796 0.027 2
LiMg2 (mp-1094593) 0.0730 0.026 2
CaMg2 (mp-1038946) 0.0715 0.110 2
Pr (mp-1059256) 0.1194 0.029 1
Rb (mp-975204) 0.1058 0.012 1
Y (mp-1059189) 0.0893 0.003 1
Sc (mp-67) 0.1224 0.000 1
Ca (mp-1064227) 0.0949 0.001 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ni_pv Mo_pv
Final Energy/Atom
-7.1396 eV
Corrected Energy
-57.1164 eV
Uncorrected energy = -57.1164 eV Corrected energy = -57.1164 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 105046
  • 644015
Submitted by
User remarks:
  • Molybdenum nickel (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)