Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.136 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.049 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.42 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ni3Sn
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 105354 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WSe2 (mp-1821) <1 1 1> <1 0 0> -0.107 175.4
GdScO3 (mp-5690) <1 0 0> <1 0 0> -0.040 140.3
WSe2 (mp-1821) <1 1 0> <1 0 0> -0.034 175.4
BaTiO3 (mp-5986) <1 0 1> <1 0 0> -0.029 70.2
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.000 315.7
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.002 60.8
GaN (mp-804) <1 0 1> <1 0 0> 0.002 210.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.003 175.4
LaF3 (mp-905) <0 0 1> <1 1 1> 0.003 182.3
SiC (mp-8062) <1 1 0> <1 1 0> 0.004 297.7
InSb (mp-20012) <1 0 0> <1 0 0> 0.008 175.4
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.012 280.6
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.016 175.4
GaN (mp-804) <0 0 1> <1 1 1> 0.018 243.0
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.020 315.7
LiF (mp-1138) <1 1 1> <1 0 0> 0.021 175.4
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.022 280.6
WS2 (mp-224) <0 0 1> <1 1 0> 0.023 248.0
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.023 248.0
Cu (mp-30) <1 1 0> <1 1 0> 0.026 148.8
Ni (mp-23) <1 1 0> <1 1 0> 0.028 297.7
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.038 175.4
Au (mp-81) <1 0 0> <1 0 0> 0.041 35.1
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.041 315.7
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.045 303.8
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.045 148.8
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.048 182.3
Au (mp-81) <1 1 0> <1 1 0> 0.048 49.6
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.051 140.3
CdS (mp-672) <0 0 1> <1 1 1> 0.062 60.8
LiF (mp-1138) <1 0 0> <1 0 0> 0.066 280.6
AlN (mp-661) <1 0 1> <1 1 0> 0.071 248.0
AlN (mp-661) <1 1 1> <1 1 0> 0.073 198.4
InP (mp-20351) <1 0 0> <1 0 0> 0.086 35.1
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.088 347.3
Al (mp-134) <1 0 0> <1 0 0> 0.090 280.6
AlN (mp-661) <1 1 0> <1 1 0> 0.093 297.7
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.094 175.4
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.095 175.4
InP (mp-20351) <1 1 0> <1 1 0> 0.100 49.6
Mg (mp-153) <0 0 1> <1 1 1> 0.102 60.8
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.103 245.6
Mg (mp-153) <1 0 1> <1 0 0> 0.104 210.5
ZnO (mp-2133) <1 0 0> <1 1 0> 0.104 347.3
InP (mp-20351) <1 1 1> <1 1 1> 0.105 60.8
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.105 347.3
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.109 175.4
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.110 175.4
Ag (mp-124) <1 0 0> <1 0 0> 0.111 35.1
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.127 140.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
149 170 170 0 0 0
170 149 170 0 0 0
170 170 149 0 0 0
0 0 0 98 0 0
0 0 0 0 98 0
0 0 0 0 0 98
Compliance Tensor Sij (10-12Pa-1)
-30.9 16.4 16.4 0 0 0
16.4 -30.9 16.4 0 0 0
16.4 16.4 -30.9 0 0 0
0 0 0 10.2 0 0
0 0 0 0 10.2 0
0 0 0 0 0 10.2
Shear Modulus GV
54 GPa
Bulk Modulus KV
163 GPa
Shear Modulus GR
-32 GPa
Bulk Modulus KR
163 GPa
Shear Modulus GVRH
11 GPa
Bulk Modulus KVRH
163 GPa
Elastic Anisotropy
-13.61
Poisson's Ratio
0.47

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Fe2CoGe (mp-30044) 0.0000 0.122 3
VCo2Si (mp-20586) 0.0000 0.027 3
ZnCo2Ge (mp-19971) 0.0000 0.000 3
CrInCo2 (mp-16735) 0.0000 0.203 3
CoCu2Sn (mp-12801) 0.0000 0.249 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.028 4
VFeCoAs (mp-1066006) 0.0000 0.221 4
VGaFeCo (mp-1066581) 0.0000 0.029 4
Na3As (mp-8860) 0.0000 0.044 2
Ca3In (mp-20581) 0.0000 0.082 2
LiIn (mp-22460) 0.0000 0.000 2
TbMg3 (mp-7381) 0.0000 0.000 2
Cs3Sb (mp-10378) 0.0000 0.000 2
Cu (mp-998890) 0.0000 0.037 1
Kr (mp-974400) 0.0000 0.002 1
H2 (mp-632250) 0.0000 2.271 1
Th (mp-11343) 0.0000 0.159 1
Ge (mp-998883) 0.0000 0.339 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ni_pv Sn_d
Final Energy/Atom
-5.4739 eV
Corrected Energy
-21.8957 eV
Uncorrected energy = -21.8957 eV Corrected energy = -21.8957 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 105354
Submitted by
User remarks:
  • Nickel tin (3/1) - HT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)