Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.502 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypePlane
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 154.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 216.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 154.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 66.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 110.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 88.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 144.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 108.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 86.6 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 207.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 88.1 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 155.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 198.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 180.1 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 108.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 86.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 242.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 129.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 207.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 154.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 154.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 286.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 129.9 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 108.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 171.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 88.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 144.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 110.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 171.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 144.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 28.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 199.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 149.2 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 72.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 43.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 144.1 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 187.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 85.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 313.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 176.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 129.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 66.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 72.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 259.8 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 180.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 149.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 66.0 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 198.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.6569 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.6143 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.6442 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.6018 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.2054 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.5563 | 0.106 | 4 |
EuAg (mp-665747) | 0.1421 | 0.000 | 2 |
LuNi (mp-1078899) | 0.1076 | 0.000 | 2 |
ErNi (mp-567314) | 0.0973 | 0.000 | 2 |
HoNi (mp-11871) | 0.0322 | 0.000 | 2 |
DyNi (mp-2738) | 0.0441 | 0.000 | 2 |
Si (mp-1001113) | 0.6855 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Ni_pv |
Final Energy/Atom-5.6292 eV |
Corrected Energy-45.0338 eV
-45.0338 eV = -45.0338 eV (uncorrected energy)
|