material

ZrOs

ID:

mp-11541

DOI:

10.17188/1188048


Tags: Osmium zirconium (1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.520 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
13.12 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 105580 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.000 45.9
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.001 21.7
Ag (mp-124) <1 0 0> <1 0 0> 0.001 86.6
ZnO (mp-2133) <1 0 1> <1 0 0> 0.006 119.1
NaCl (mp-22862) <1 1 1> <1 1 1> 0.009 56.3
NaCl (mp-22862) <1 1 0> <1 1 0> 0.009 45.9
TePb (mp-19717) <1 1 1> <1 1 1> 0.026 75.0
TePb (mp-19717) <1 1 0> <1 1 0> 0.026 61.2
Au (mp-81) <1 0 0> <1 0 0> 0.027 86.6
Al (mp-134) <1 1 0> <1 1 0> 0.027 45.9
TePb (mp-19717) <1 0 0> <1 0 0> 0.027 43.3
SiC (mp-7631) <1 1 1> <1 1 0> 0.028 245.0
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.042 168.4
Si (mp-149) <1 0 0> <1 0 0> 0.043 270.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.050 270.7
WS2 (mp-224) <0 0 1> <1 1 1> 0.074 168.8
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.075 168.8
GaP (mp-2490) <1 0 0> <1 0 0> 0.090 270.7
InP (mp-20351) <1 1 1> <1 1 1> 0.093 243.8
InP (mp-20351) <1 0 0> <1 0 0> 0.096 140.8
Al (mp-134) <1 1 1> <1 0 0> 0.111 227.4
SiC (mp-7631) <1 0 1> <1 1 0> 0.117 336.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.118 43.3
LaAlO3 (mp-2920) <1 0 0> <1 1 0> 0.123 214.4
ZnO (mp-2133) <1 0 0> <1 0 0> 0.124 86.6
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.125 122.5
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.132 61.2
Ni (mp-23) <1 1 0> <1 1 0> 0.143 137.8
Ni (mp-23) <1 0 0> <1 0 0> 0.146 97.4
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.153 168.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.154 54.1
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.157 45.9
CdS (mp-672) <1 1 1> <1 1 1> 0.164 262.5
AlN (mp-661) <1 0 0> <1 0 0> 0.176 140.8
Cu (mp-30) <1 1 0> <1 1 0> 0.183 168.4
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.184 131.3
Mg (mp-153) <0 0 1> <1 1 1> 0.184 168.8
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.187 270.7
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.195 227.4
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.201 45.9
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.201 86.6
SiC (mp-8062) <1 1 1> <1 1 1> 0.202 131.3
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.225 194.9
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.227 260.3
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.229 275.6
ZnO (mp-2133) <0 0 1> <1 0 0> 0.230 75.8
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.260 75.8
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.263 75.8
NaCl (mp-22862) <1 0 0> <1 1 0> 0.267 229.7
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.270 75.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
357 135 135 0 0 0
135 357 135 0 0 0
135 135 357 0 0 0
0 0 0 91 0 0
0 0 0 0 91 0
0 0 0 0 0 91
Compliance Tensor Sij (10-12Pa-1)
3.5 -1 -1 0 0 0
-1 3.5 -1 0 0 0
-1 -1 3.5 0 0 0
0 0 0 10.9 0 0
0 0 0 0 10.9 0
0 0 0 0 0 10.9
Shear Modulus GV
99 GPa
Bulk Modulus KV
209 GPa
Shear Modulus GR
98 GPa
Bulk Modulus KR
209 GPa
Shear Modulus GVRH
99 GPa
Bulk Modulus KVRH
209 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
HoTmZn2 (mp-983126) 0.0000 0.000 3
Pm2PtAu (mp-982772) 0.0000 0.000 3
Nd2IrAu (mp-973606) 0.0000 0.063 3
YbPrPd2 (mp-981530) 0.0000 0.007 3
YTmAl2 (mp-980662) 0.0000 0.016 3
TiFeCoSb (mp-998973) 0.0000 0.186 4
TiAlFeCo (mp-998980) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.028 4
VFeCoSi (mp-1066609) 0.0000 0.002 4
VFeCoSb (mp-1066862) 0.0000 0.164 4
ErPd (mp-851) 0.0000 0.000 2
YbRu (mp-567116) 0.0000 0.228 2
PrIn (mp-20023) 0.0000 0.000 2
ReC (mp-1009731) 0.0000 1.115 2
ScCu (mp-1169) 0.0000 0.000 2
Cu (mp-998890) 0.0000 0.037 1
Kr (mp-974400) 0.0000 0.002 1
H2 (mp-632250) 0.0000 0.000 1
Ge (mp-998883) 0.0000 0.340 1
U (mp-108) 0.0000 0.271 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Os_pv
Final Energy/Atom
-10.4077 eV
Corrected Energy
-20.8155 eV
Uncorrected energy = -20.8155 eV Corrected energy = -20.8155 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 105580
  • 290934
Submitted by
User remarks:
  • Osmium zirconium (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)