material

Zr2Fe

ID:

mp-1159

DOI:

10.17188/1188091


Tags: Iron zirconium (1/2) Iron zirconium hydride (2/4/9)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.135 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.00 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Zr3Fe + ZrFe2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 103712 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaF3 (mp-905) <1 0 0> <1 1 1> 0.001 321.7
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.008 324.1
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.008 157.3
GaSe (mp-1943) <1 0 0> <1 1 0> 0.009 203.7
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.010 360.2
MoSe2 (mp-1634) <0 0 1> <1 1 0> 0.014 152.8
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.014 39.3
WSe2 (mp-1821) <0 0 1> <1 1 0> 0.015 152.8
C (mp-48) <1 1 0> <1 0 1> 0.016 266.6
Au (mp-81) <1 0 0> <0 0 1> 0.017 157.3
InSb (mp-20012) <1 0 0> <0 0 1> 0.026 353.9
GaN (mp-804) <0 0 1> <0 0 1> 0.028 314.6
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.032 275.2
CdTe (mp-406) <1 0 0> <0 0 1> 0.039 353.9
TiO2 (mp-390) <1 0 1> <1 0 0> 0.047 360.2
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.049 305.6
BN (mp-984) <1 0 0> <1 0 0> 0.061 288.1
MoSe2 (mp-1634) <1 1 1> <1 0 0> 0.065 180.1
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.068 196.6
Cu (mp-30) <1 1 0> <0 0 1> 0.072 275.2
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.081 196.6
Ag (mp-124) <1 0 0> <0 0 1> 0.082 157.3
ZnO (mp-2133) <1 1 0> <1 1 0> 0.104 152.8
C (mp-48) <0 0 1> <1 0 0> 0.110 180.1
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.110 314.6
Te2W (mp-22693) <1 0 0> <0 0 1> 0.113 196.6
CdS (mp-672) <1 0 0> <1 0 1> 0.128 319.9
C (mp-48) <1 1 1> <1 0 1> 0.140 266.6
AlN (mp-661) <1 1 1> <1 1 0> 0.145 254.7
LaF3 (mp-905) <0 0 1> <0 0 1> 0.147 314.6
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.147 235.9
LiF (mp-1138) <1 1 1> <1 0 1> 0.151 319.9
Cu (mp-30) <1 0 0> <1 0 0> 0.167 252.1
LaAlO3 (mp-2920) <1 1 1> <1 1 0> 0.168 254.7
PbSe (mp-2201) <1 0 0> <0 0 1> 0.176 39.3
CaCO3 (mp-3953) <1 1 0> <1 1 0> 0.177 152.8
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.179 213.3
MoSe2 (mp-1634) <1 1 0> <1 0 0> 0.184 180.1
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.185 252.1
Ni (mp-23) <1 1 0> <1 1 1> 0.191 193.0
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.192 157.3
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.198 275.2
AlN (mp-661) <0 0 1> <0 0 1> 0.204 275.2
InP (mp-20351) <1 0 0> <0 0 1> 0.210 314.6
Ni (mp-23) <1 1 1> <1 0 0> 0.211 252.1
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.214 72.0
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.215 118.0
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.220 196.6
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.223 288.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.231 288.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
200 75 75 0 0 0
75 178 132 0 0 0
75 132 178 0 0 0
0 0 0 36 0 0
0 0 0 0 24 0
0 0 0 0 0 24
Compliance Tensor Sij (10-12Pa-1)
6.1 -1.5 -1.5 0 0 0
-1.5 12.9 -9 0 0 0
-1.5 -9 12.9 0 0 0
0 0 0 28 0 0
0 0 0 0 40.8 0
0 0 0 0 0 40.8
Shear Modulus GV
35 GPa
Bulk Modulus KV
125 GPa
Shear Modulus GR
30 GPa
Bulk Modulus KR
124 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
124 GPa
Elastic Anisotropy
0.92
Poisson's Ratio
0.38

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.5697 0.044 3
Nb4SiNi (mp-22396) 0.5353 0.009 3
Ta4FeP (mp-22444) 0.5851 0.055 3
Nb4CoSi (mp-10003) 0.6029 0.013 3
Zr4CuP (mp-581733) 0.5722 0.063 3
Zr2Co (mp-628) 0.3732 0.000 2
Mg2Pt (mp-13208) 0.3641 0.000 2
Zr2Ir (mp-1077297) 0.3106 0.000 2
Sc2Co (mp-30562) 0.1561 0.011 2
In2Ir (mp-22812) 0.4372 0.000 2
Bi (mp-1078637) 0.7441 0.097 1
Si (mp-1079649) 0.7416 0.426 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Fe_pv
Final Energy/Atom
-8.6566 eV
Corrected Energy
-51.9395 eV
-51.9395 eV = -51.9395 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 634192
  • 634145
  • 656524
  • 634183
  • 634154
  • 103712
Submitted by
User remarks:
  • Iron zirconium (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)