material

ThC

ID:

mp-1164

DOI:

10.17188/1188121


Tags: Thorium carbide (1/1) Thorium carbide Thorium carbide (2.66/5.32)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.276 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.56 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 43378 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.000 162.3
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.000 198.8
Ni (mp-23) <1 1 1> <1 1 1> 0.000 149.1
InAs (mp-20305) <1 1 0> <1 1 0> 0.002 162.3
InAs (mp-20305) <1 1 1> <1 1 1> 0.002 198.8
TePb (mp-19717) <1 1 0> <1 1 0> 0.003 121.7
C (mp-66) <1 0 0> <1 0 0> 0.003 114.8
C (mp-66) <1 1 0> <1 1 0> 0.004 162.3
CdS (mp-672) <0 0 1> <1 1 1> 0.004 198.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.007 81.2
SiC (mp-7631) <1 1 0> <1 1 0> 0.009 81.2
SiC (mp-11714) <1 1 0> <1 1 0> 0.012 162.3
NaCl (mp-22862) <1 0 0> <1 0 0> 0.012 258.3
GaN (mp-804) <0 0 1> <1 1 1> 0.018 347.9
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.019 229.6
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.021 143.5
PbS (mp-21276) <1 0 0> <1 0 0> 0.022 143.5
Al (mp-134) <1 1 1> <1 1 1> 0.026 198.8
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.027 198.8
ZnO (mp-2133) <0 0 1> <1 1 1> 0.028 149.1
TiO2 (mp-2657) <1 1 1> <1 1 1> 0.031 347.9
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.034 114.8
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.041 258.3
CdSe (mp-2691) <1 1 0> <1 1 0> 0.077 162.3
CdSe (mp-2691) <1 1 1> <1 1 1> 0.078 198.8
SiC (mp-11714) <1 0 0> <1 1 0> 0.080 284.1
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.083 198.8
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.086 114.8
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.087 162.3
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.088 198.8
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.090 229.6
TiO2 (mp-390) <0 0 1> <1 0 0> 0.090 28.7
ZnO (mp-2133) <1 1 0> <1 1 0> 0.099 121.7
MgO (mp-1265) <1 0 0> <1 0 0> 0.100 143.5
InP (mp-20351) <1 0 0> <1 0 0> 0.112 143.5
SiC (mp-7631) <0 0 1> <1 0 0> 0.116 200.9
GaSb (mp-1156) <1 1 0> <1 1 0> 0.117 162.3
GaSb (mp-1156) <1 1 1> <1 1 1> 0.118 198.8
TePb (mp-19717) <1 0 0> <1 1 1> 0.119 347.9
SiC (mp-11714) <0 0 1> <1 0 0> 0.126 200.9
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.129 258.3
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.130 229.6
TiO2 (mp-2657) <1 1 0> <1 1 1> 0.130 347.9
BN (mp-984) <1 1 1> <1 1 0> 0.132 202.9
WS2 (mp-224) <0 0 1> <1 1 1> 0.135 347.9
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.137 347.9
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.140 200.9
Mg (mp-153) <1 0 1> <1 1 0> 0.155 284.1
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.156 198.8
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.158 198.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
226 95 95 0 0 0
95 226 95 0 0 0
95 95 226 0 0 0
0 0 0 79 0 0
0 0 0 0 79 0
0 0 0 0 0 79
Compliance Tensor Sij (10-12Pa-1)
5.9 -1.7 -1.7 0 0 0
-1.7 5.9 -1.7 0 0 0
-1.7 -1.7 5.9 0 0 0
0 0 0 12.6 0 0
0 0 0 0 12.6 0
0 0 0 0 0 12.6
Shear Modulus GV
74 GPa
Bulk Modulus KV
139 GPa
Shear Modulus GR
73 GPa
Bulk Modulus KR
139 GPa
Shear Modulus GVRH
73 GPa
Bulk Modulus KVRH
139 GPa
Elastic Anisotropy
0.04
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.114 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
TiH (mp-1060435) 0.0000 0.045 2
USe (mp-911057) 0.0000 0.000 2
TcC (mp-1009876) 0.0000 0.650 2
TcC (mp-1009837) 0.0000 0.650 2
MgCd (mp-1039157) 0.0000 0.249 2
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Na (mp-1093989) 0.0000 1.084 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Th C
Final Energy/Atom
-8.5967 eV
Corrected Energy
-17.1933 eV
Uncorrected energy = -17.1933 eV Corrected energy = -17.1933 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 618902
  • 618907
  • 260883
  • 618908
  • 618913
  • 618905
  • 618894
  • 43378
  • 290715
  • 618899
  • 618904
  • 618910
Submitted by
User remarks:
  • Thorium carbide (1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)