Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.479 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
InSb (mp-20012) | <1 0 0> | <1 0 0> | 0.000 | 88.0 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 0.000 | 124.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 0.001 | 88.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 0.001 | 124.4 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 0.002 | 88.0 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 0.008 | 55.3 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 0.008 | 67.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 0.009 | 78.2 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 0.010 | 127.1 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 0.010 | 205.3 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 0.013 | 203.2 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 0.017 | 221.2 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 0.019 | 152.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 0.020 | 107.5 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 0.021 | 195.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 0.024 | 127.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 0.024 | 50.8 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 0.027 | 262.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 0.031 | 48.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 0.032 | 124.4 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 0.034 | 244.4 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 0.042 | 176.0 |
BN (mp-984) | <1 0 0> | <1 1 1> | 0.043 | 135.4 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 0.043 | 39.1 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 0.045 | 55.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 0.046 | 156.4 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 0.046 | 67.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 0.048 | 270.9 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 0.053 | 244.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 0.054 | 124.4 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 0.055 | 67.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 0.056 | 67.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 0.057 | 39.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 0.060 | 55.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 0.061 | 67.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 0.065 | 127.1 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 0.065 | 152.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 0.070 | 68.4 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 0.072 | 39.1 |
Au (mp-81) | <1 0 0> | <1 0 0> | 0.076 | 88.0 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 0.076 | 55.3 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 0.077 | 29.3 |
MgF2 (mp-1249) | <1 1 0> | <1 1 0> | 0.078 | 41.5 |
GaSb (mp-1156) | <1 1 1> | <1 1 1> | 0.078 | 67.7 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 0.078 | 152.1 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 0.093 | 118.5 |
CaCO3 (mp-3953) | <1 0 1> | <1 1 1> | 0.094 | 270.9 |
C (mp-48) | <0 0 1> | <1 1 1> | 0.095 | 67.7 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 0.101 | 39.1 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 0.104 | 67.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
171 | 86 | 86 | 0 | 0 | 0 |
86 | 171 | 86 | 0 | 0 | 0 |
86 | 86 | 171 | 0 | 0 | 0 |
0 | 0 | 0 | 71 | 0 | 0 |
0 | 0 | 0 | 0 | 71 | 0 |
0 | 0 | 0 | 0 | 0 | 71 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.8 | -2.9 | -2.9 | 0 | 0 | 0 |
-2.9 | 8.8 | -2.9 | 0 | 0 | 0 |
-2.9 | -2.9 | 8.8 | 0 | 0 | 0 |
0 | 0 | 0 | 14 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | 0 |
0 | 0 | 0 | 0 | 0 | 14 |
Shear Modulus GV60 GPa |
Bulk Modulus KV115 GPa |
Shear Modulus GR56 GPa |
Bulk Modulus KR115 GPa |
Shear Modulus GVRH58 GPa |
Bulk Modulus KVRH115 GPa |
Elastic Anisotropy0.33 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
Nd2IrAu (mp-973606) | 0.0000 | 0.063 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.007 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.228 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Rh_pv |
Final Energy/Atom-4.9472 eV |
Corrected Energy-9.8943 eV
-9.8943 eV = -9.8943 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)