material

CaSn2Rh

ID:

mp-11959

DOI:

10.17188/1188483


Tags: Calcium rhodium stannide (1/1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.671 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.92 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 410775 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.010 250.6
CdSe (mp-2691) <1 1 1> <0 1 0> 0.011 66.8
GaSe (mp-1943) <1 0 0> <1 1 0> 0.013 269.9
GaSb (mp-1156) <1 1 1> <0 1 0> 0.019 66.8
CdS (mp-672) <0 0 1> <0 1 0> 0.020 200.3
C (mp-66) <1 1 1> <0 1 0> 0.021 66.8
CaCO3 (mp-3953) <0 0 1> <0 1 0> 0.029 66.8
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.030 250.6
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.030 66.8
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.030 66.8
BN (mp-984) <1 1 0> <0 1 0> 0.032 33.4
BaTiO3 (mp-5986) <1 0 1> <0 1 0> 0.033 233.6
ZnTe (mp-2176) <1 1 1> <0 1 0> 0.037 66.8
PbSe (mp-2201) <1 1 1> <0 1 0> 0.037 66.8
TiO2 (mp-2657) <1 1 0> <0 1 0> 0.038 233.6
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.038 167.1
Cu (mp-30) <1 1 0> <1 0 0> 0.043 167.1
InAs (mp-20305) <1 1 1> <0 1 0> 0.046 66.8
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.047 239.2
BN (mp-984) <0 0 1> <0 0 1> 0.048 143.5
AlN (mp-661) <0 0 1> <0 0 1> 0.058 239.2
InSb (mp-20012) <1 1 0> <1 0 0> 0.060 250.6
GaSe (mp-1943) <0 0 1> <0 1 0> 0.061 100.1
CdS (mp-672) <1 0 0> <1 0 1> 0.062 288.8
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.063 334.9
MgAl2O4 (mp-3536) <1 1 1> <0 1 0> 0.064 233.6
PbSe (mp-2201) <1 0 0> <0 1 1> 0.067 116.7
CdTe (mp-406) <1 1 0> <1 0 0> 0.069 250.6
LiF (mp-1138) <1 1 1> <0 1 0> 0.074 200.3
GaSb (mp-1156) <1 0 0> <0 1 1> 0.075 116.7
Au (mp-81) <1 0 0> <0 1 1> 0.077 175.0
ZrO2 (mp-2858) <1 0 0> <1 0 1> 0.078 288.8
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 0.079 143.5
TiO2 (mp-390) <0 0 1> <0 1 0> 0.081 233.6
CdTe (mp-406) <1 0 0> <0 1 1> 0.084 175.0
CdSe (mp-2691) <1 0 0> <0 1 1> 0.087 116.7
Mg (mp-153) <1 1 1> <0 0 1> 0.088 239.2
InSb (mp-20012) <1 0 0> <0 1 1> 0.093 175.0
Al (mp-134) <1 1 1> <0 1 0> 0.094 200.3
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.094 200.3
CeO2 (mp-20194) <1 1 0> <1 0 0> 0.103 83.5
MgF2 (mp-1249) <0 0 1> <0 1 1> 0.107 175.0
Si (mp-149) <1 1 0> <1 0 0> 0.109 83.5
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.110 179.9
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.115 96.3
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.116 175.0
Ag (mp-124) <1 0 0> <0 1 1> 0.117 175.0
SiO2 (mp-6930) <1 1 1> <0 1 0> 0.128 267.0
Cu (mp-30) <1 0 0> <0 0 1> 0.129 239.2
LaAlO3 (mp-2920) <1 1 0> <1 0 0> 0.142 250.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
91 39 72 0 0 0
39 99 36 0 0 0
72 36 120 0 0 0
0 0 0 29 0 0
0 0 0 0 59 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
22.7 -4.5 -12.3 0 0 0
-4.5 12.2 -0.9 0 0 0
-12.3 -0.9 16 0 0 0
0 0 0 34.9 0 0
0 0 0 0 16.9 0
0 0 0 0 0 29.5
Shear Modulus GV
35 GPa
Bulk Modulus KV
67 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
65 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
66 GPa
Elastic Anisotropy
1.12
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YIn2Ni (mp-22056) 0.1895 0.000 3
CaSn2Ir (mp-11957) 0.1010 0.000 3
EuSn2Ir (mp-22742) 0.2094 0.000 3
DyIn2Ni (mp-1079916) 0.2478 0.000 3
CaIn2Cu (mp-19968) 0.1942 0.012 3
LiYb2InGe2 (mp-977355) 0.7005 0.000 4
Sr2LiInGe2 (mp-571617) 0.7055 0.000 4
LiCa2InGe2 (mp-570850) 0.6922 0.000 4
KSi (mp-1217) 0.6222 0.000 2
MgH2 (mp-23712) 0.6083 0.082 2
KGe (mp-2146) 0.5948 0.041 2
RbGe (mp-1888) 0.6257 0.038 2
CsSn (mp-571056) 0.5822 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Sn_d Rh_pv
Final Energy/Atom
-5.0015 eV
Corrected Energy
-40.0120 eV
Uncorrected energy = -40.0120 eV Corrected energy = -40.0120 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 410775
Submitted by
User remarks:
  • Calcium rhodium stannide (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)