material

YMgTl

ID:

mp-11984

DOI:

10.17188/1188492


Tags: High pressure experimental phase Yttrium magnesium thallide

Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.349 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.80 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P62m [189]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.000 198.8
Ni (mp-23) <1 1 1> <0 0 1> 0.000 149.1
InAs (mp-20305) <1 1 1> <0 0 1> 0.001 198.8
CdS (mp-672) <0 0 1> <0 0 1> 0.002 198.8
SiC (mp-8062) <1 1 0> <1 0 1> 0.003 244.2
NaCl (mp-22862) <1 1 0> <1 0 1> 0.003 183.1
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.004 283.6
SiC (mp-7631) <1 1 0> <1 0 1> 0.006 244.2
ZnO (mp-2133) <1 0 0> <0 0 1> 0.007 347.9
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.010 183.1
Al (mp-134) <1 1 1> <0 0 1> 0.013 198.8
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.013 198.8
ZnO (mp-2133) <1 1 1> <1 0 0> 0.013 283.6
ZnO (mp-2133) <0 0 1> <0 0 1> 0.015 149.1
Cu (mp-30) <1 1 0> <1 1 1> 0.024 316.0
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.027 122.8
AlN (mp-661) <1 0 0> <1 0 0> 0.029 141.8
Al (mp-134) <1 1 0> <1 0 1> 0.035 183.1
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.036 177.2
CdSe (mp-2691) <1 1 1> <0 0 1> 0.040 198.8
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.041 198.8
SiC (mp-7631) <1 0 0> <1 0 0> 0.042 141.8
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.043 198.8
ZrO2 (mp-2858) <0 1 0> <1 0 1> 0.044 305.2
ZnO (mp-2133) <1 0 1> <1 0 0> 0.045 177.2
TiO2 (mp-390) <1 0 1> <1 0 0> 0.047 319.0
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.050 177.2
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.053 319.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.061 198.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.067 347.9
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.067 347.9
BN (mp-984) <1 0 1> <1 0 1> 0.070 61.0
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.071 305.2
SiC (mp-11714) <1 0 0> <1 0 0> 0.071 248.1
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.073 106.3
AlN (mp-661) <1 1 0> <1 0 1> 0.077 244.2
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.080 198.8
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.081 198.8
CdTe (mp-406) <1 0 0> <0 0 1> 0.088 347.9
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.091 319.0
PbSe (mp-2201) <1 1 1> <0 0 1> 0.092 198.8
C (mp-48) <0 0 1> <1 0 0> 0.095 354.5
TiO2 (mp-390) <1 0 0> <0 0 1> 0.102 149.1
InSb (mp-20012) <1 0 0> <0 0 1> 0.102 347.9
Ni (mp-23) <1 1 0> <0 0 1> 0.120 347.9
CdTe (mp-406) <1 1 0> <0 0 1> 0.120 248.5
InSb (mp-20012) <1 1 0> <0 0 1> 0.122 248.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.127 49.7
LiGaO2 (mp-5854) <1 1 0> <1 0 1> 0.135 244.2
InAs (mp-20305) <1 0 0> <1 0 1> 0.138 305.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
98 27 35 0 0 0
27 98 35 0 0 0
35 35 96 0 0 0
0 0 0 50 0 0
0 0 0 0 50 0
0 0 0 0 0 35
Compliance Tensor Sij (10-12Pa-1)
12.1 -2 -3.7 0 0 0
-2 12.1 -3.7 0 0 0
-3.7 -3.7 13.1 0 0 0
0 0 0 20.2 0 0
0 0 0 0 20.2 0
0 0 0 0 0 28.2
Shear Modulus GV
40 GPa
Bulk Modulus KV
54 GPa
Shear Modulus GR
38 GPa
Bulk Modulus KR
54 GPa
Shear Modulus GVRH
39 GPa
Bulk Modulus KVRH
54 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiCa2InGe2 (mp-570850) 0.4281 0.000 4
Yb2LiInGe2 (mp-977355) 0.4291 0.000 4
Sr2LiInGe2 (mp-571617) 0.3612 0.000 4
Yb3In3Ge2Au (mp-981207) 0.2588 0.000 4
Er5Al3Ni3Ge4 (mp-638521) 0.5951 0.000 4
Ni2P (mp-21167) 0.6055 0.003 2
BaCl2 (mp-567680) 0.5244 0.030 2
BaI2 (mp-568536) 0.5793 0.006 2
Ni4B3 (mp-640067) 0.5484 0.000 2
Fe2P (mp-778) 0.4529 0.000 2
SmMgIn (mp-21456) 0.0190 0.000 3
ScSiCu (mp-15322) 0.0327 0.000 3
SmMgTl (mp-11987) 0.0517 0.000 3
YMgIn (mp-21503) 0.0660 0.000 3
YMgAl (mp-13090) 0.0459 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv Y_sv Tl_d
Final Energy/Atom
-3.8270 eV
Corrected Energy
-34.4428 eV
-34.4428 eV = -34.4428 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 414438
Submitted by
User remarks:
  • High pressure experimental phase
  • Yttrium magnesium thallide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)