Final Magnetic Moment0.013 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.075 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 24.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 141.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 74.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 120.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 80.6 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 197.5 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 40.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 128.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 181.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 172.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 356.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 161.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 156.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 85.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 213.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 60.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 285.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 296.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 362.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 313.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 161.3 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 123.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 60.5 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 74.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 60.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 262.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 161.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 181.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 213.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 128.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 270.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.3 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 322.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 128.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 181.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 172.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 128.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 181.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 320.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 123.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 24.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 141.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 181.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 28.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 256.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 213.8 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 342.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 285.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
50 | 44 | 44 | 0 | 0 | 0 |
44 | 50 | 44 | 0 | 0 | 0 |
44 | 44 | 50 | 0 | 0 | 0 |
0 | 0 | 0 | 39 | 0 | 0 |
0 | 0 | 0 | 0 | 39 | 0 |
0 | 0 | 0 | 0 | 0 | 39 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
107.4 | -50.1 | -50.1 | 0 | 0 | 0 |
-50.1 | 107.4 | -50.1 | 0 | 0 | 0 |
-50.1 | -50.1 | 107.4 | 0 | 0 | 0 |
0 | 0 | 0 | 25.4 | 0 | 0 |
0 | 0 | 0 | 0 | 25.4 | 0 |
0 | 0 | 0 | 0 | 0 | 25.4 |
Shear Modulus GV25 GPa |
Bulk Modulus KV46 GPa |
Shear Modulus GR7 GPa |
Bulk Modulus KR46 GPa |
Shear Modulus GVRH16 GPa |
Bulk Modulus KVRH46 GPa |
Elastic Anisotropy12.55 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
Nd2IrAu (mp-973606) | 0.0000 | 0.063 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.007 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.228 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Mg_pv |
Final Energy/Atom-3.1649 eV |
Corrected Energy-6.3298 eV
-6.3298 eV = -6.3298 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)