material

CrIr3

ID:

mp-12083

DOI:

10.17188/1188560


Tags: Chromium iridium (1/3)

Material Details

Final Magnetic Moment
1.181 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-0.241 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
18.65 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 626213 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.001 25.3
CdTe (mp-406) <1 1 0> <1 1 0> 0.002 62.1
CdTe (mp-406) <1 1 1> <1 1 1> 0.002 76.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.004 131.7
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.004 186.3
InSb (mp-20012) <1 1 0> <1 1 0> 0.009 62.1
InSb (mp-20012) <1 1 1> <1 1 1> 0.009 76.0
AlN (mp-661) <0 0 1> <1 1 1> 0.019 25.3
GaAs (mp-2534) <1 0 0> <1 0 0> 0.028 131.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.030 186.3
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.036 73.2
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.046 76.0
C (mp-48) <1 0 1> <1 0 0> 0.046 219.5
Cu (mp-30) <1 0 0> <1 0 0> 0.047 117.1
Cu (mp-30) <1 1 0> <1 1 0> 0.050 165.6
LaAlO3 (mp-2920) <1 1 1> <1 1 1> 0.054 126.7
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.063 124.2
PbSe (mp-2201) <1 1 0> <1 1 0> 0.068 165.6
ZnO (mp-2133) <1 0 1> <1 0 0> 0.084 219.5
GaSe (mp-1943) <1 0 0> <1 0 0> 0.102 204.9
Ge (mp-32) <1 0 0> <1 0 0> 0.119 131.7
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.124 278.0
Ge (mp-32) <1 1 0> <1 1 0> 0.127 186.3
Al (mp-134) <1 0 0> <1 0 0> 0.130 131.7
GaSb (mp-1156) <1 1 0> <1 1 0> 0.132 165.6
Al (mp-134) <1 1 0> <1 1 0> 0.139 186.3
MgO (mp-1265) <1 0 0> <1 0 0> 0.143 73.2
TiO2 (mp-390) <0 0 1> <1 0 0> 0.158 14.6
C (mp-48) <1 1 1> <1 0 0> 0.160 336.6
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.162 76.0
TeO2 (mp-2125) <1 0 1> <1 0 0> 0.191 307.3
DyScO3 (mp-31120) <0 1 0> <1 1 1> 0.193 304.1
CdSe (mp-2691) <1 1 0> <1 1 0> 0.198 165.6
InSb (mp-20012) <1 0 0> <1 1 0> 0.206 310.4
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.210 62.1
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.229 165.6
CdTe (mp-406) <1 0 0> <1 1 0> 0.240 310.4
C (mp-48) <0 0 1> <1 1 1> 0.247 101.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.261 131.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.268 131.7
BN (mp-984) <1 1 0> <1 1 0> 0.279 165.6
LiF (mp-1138) <1 1 0> <1 1 0> 0.279 186.3
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.281 82.8
MgO (mp-1265) <1 1 0> <1 1 0> 0.284 227.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.287 186.3
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.302 131.7
SiC (mp-7631) <1 1 1> <1 0 0> 0.305 248.8
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.322 186.3
InAs (mp-20305) <1 1 1> <1 1 0> 0.335 331.1
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.340 219.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
521 200 200 0 0 0
200 521 200 0 0 0
200 200 521 0 0 0
0 0 0 259 0 0
0 0 0 0 259 0
0 0 0 0 0 259
Compliance Tensor Sij (10-12Pa-1)
2.4 -0.7 -0.7 0 0 0
-0.7 2.4 -0.7 0 0 0
-0.7 -0.7 2.4 0 0 0
0 0 0 3.9 0 0
0 0 0 0 3.9 0
0 0 0 0 0 3.9
Shear Modulus GV
220 GPa
Bulk Modulus KV
307 GPa
Shear Modulus GR
208 GPa
Bulk Modulus KR
307 GPa
Shear Modulus GVRH
214 GPa
Bulk Modulus KVRH
307 GPa
Elastic Anisotropy
0.28
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.034 3
LiCa6Ge (mp-12609) 0.0000 0.183 3
GaFeNi2 (mp-1065359) 0.0412 0.065 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.065 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
YPd3 (mp-559) 0.0000 0.000 2
DySn3 (mp-570860) 0.0000 0.033 2
HfAl3 (mp-1007730) 0.0000 0.023 2
ThRh3 (mp-2509) 0.0000 0.000 2
TiZn3 (mp-21289) 0.0000 0.000 2
Na (mp-974558) 0.0000 0.003 1
Br (mp-998870) 0.0000 0.666 1
Mn (mp-8634) 0.0000 0.083 1
Pb (mp-20483) 0.0000 0.000 1
Cu (mp-30) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cr_pv Ir
Final Energy/Atom
-9.2827 eV
Corrected Energy
-37.1307 eV
-37.1307 eV = -37.1307 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 626213
Submitted by
User remarks:
  • Chromium iridium (1/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)