Final Magnetic Moment1.031 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.425 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.104 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr3Si + CrSi2 + LuSi |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 128.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 161.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 176.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 282.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 87.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 121.3 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 128.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 43.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 159.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 202.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 188.7 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 57.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 188.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 171.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 257.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 121.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 171.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 261.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 214.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 128.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 275.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 188.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 159.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 217.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 72.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 161.7 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 323.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 323.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 319.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 145.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 161.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 128.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 171.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 128.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 242.5 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 214.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 282.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 290.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 130.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 285.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 202.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 161.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 290.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 246.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 319.3 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 228.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 121.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 202.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 161.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ho(CrSi)2 (mp-5561) | 0.0447 | 0.110 | 3 |
Tm(CrSi)2 (mp-567243) | 0.0213 | 0.105 | 3 |
Y(CrSi)2 (mp-4740) | 0.0640 | 0.121 | 3 |
Dy(CrSi)2 (mp-19909) | 0.0569 | 0.113 | 3 |
Er(CrSi)2 (mp-12082) | 0.0307 | 0.108 | 3 |
NdAl4 (mp-1834) | 0.2964 | 0.058 | 2 |
NaGa4 (mp-454) | 0.3424 | 0.000 | 2 |
PrAl4 (mp-2336) | 0.3356 | 0.037 | 2 |
CeAl4 (mp-2289) | 0.2646 | 0.040 | 2 |
SmAl4 (mp-1891) | 0.2323 | 0.078 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Cr_pv Si |
Final Energy/Atom-7.3593 eV |
Corrected Energy-36.6546 eV
Uncorrected energy = -36.7966 eV
Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV
Corrected energy = -36.6546 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)