Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.179 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6/mmm [191] |
Hall-P 6 2 |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 230.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 160.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 115.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 137.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 139.2 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 86.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 259.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 226.2 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 144.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 191.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 87.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 23.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 252.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 206.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 317.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 241.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 206.7 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 113.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 261.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 91.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 226.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 174.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 331.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 261.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 313.1 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 230.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 174.0 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 144.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 261.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.9 |
GaSe (mp-1943) | <1 0 1> | <1 0 1> | 201.7 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 120.5 |
GaSe (mp-1943) | <1 1 1> | <1 1 0> | 120.5 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 210.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 115.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 156.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 87.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 150.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 160.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 259.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 301.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 271.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
122 | 43 | 43 | 0 | 0 | 0 |
43 | 122 | 43 | 0 | 0 | 0 |
43 | 43 | 94 | 0 | 0 | 0 |
0 | 0 | 0 | 36 | 0 | 0 |
0 | 0 | 0 | 0 | 36 | 0 |
0 | 0 | 0 | 0 | 0 | 39 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
10.3 | -2.4 | -3.6 | 0 | 0 | 0 |
-2.4 | 10.3 | -3.6 | 0 | 0 | 0 |
-3.6 | -3.6 | 13.9 | 0 | 0 | 0 |
0 | 0 | 0 | 28 | 0 | 0 |
0 | 0 | 0 | 0 | 28 | 0 |
0 | 0 | 0 | 0 | 0 | 25.5 |
Shear Modulus GV36 GPa |
Bulk Modulus KV66 GPa |
Shear Modulus GR36 GPa |
Bulk Modulus KR65 GPa |
Shear Modulus GVRH36 GPa |
Bulk Modulus KVRH65 GPa |
Elastic Anisotropy0.08 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAlPt (mp-1025063) | 0.0441 | 0.102 | 3 |
MnNiGe (mp-21090) | 0.1089 | 0.030 | 3 |
MnNiGe (mp-583202) | 0.1053 | 0.323 | 3 |
TiAlAu (mp-16481) | 0.1089 | 0.000 | 3 |
LiSnAu (mp-11977) | 0.1243 | 0.001 | 3 |
Rb2Te (mp-383) | 0.1074 | 0.057 | 2 |
Li2Pd (mp-728) | 0.1089 | 0.000 | 2 |
Yb2Sn (mp-570050) | 0.0150 | 0.000 | 2 |
Mg2Si (mp-1018796) | 0.0028 | 0.160 | 2 |
Li2Pt (mp-2170) | 0.0318 | 0.000 | 2 |
Ti (mp-72) | 0.4525 | 0.000 | 1 |
Hf (mp-1009460) | 0.4632 | 0.045 | 1 |
Hg (mp-10861) | 0.7341 | 0.003 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Cd |
Final Energy/Atom-3.2658 eV |
Corrected Energy-9.7973 eV
-9.7973 eV = -9.7973 eV (uncorrected energy)
|