Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.985 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2Sb4O11 + KSbO3 |
Band Gap1.199 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbam [55] |
Hall-P 2 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 0 0> | <0 0 1> | 217.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 217.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 325.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 184.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 217.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 217.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 187.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 271.3 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 271.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 271.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 217.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 192.0 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 217.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 325.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 325.6 |
C (mp-66) | <1 0 0> | <0 1 0> | 179.7 |
C (mp-66) | <1 1 0> | <0 1 0> | 179.7 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 108.5 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 179.7 |
LaF3 (mp-905) | <1 1 0> | <0 1 0> | 179.7 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 54.3 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 325.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 325.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 217.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 271.3 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 325.6 |
Au (mp-81) | <1 1 0> | <0 0 1> | 217.1 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 325.6 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 217.1 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 54.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 271.3 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 271.3 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 54.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 192.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 162.8 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 179.7 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 162.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 162.8 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 271.3 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 325.6 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 54.3 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 184.2 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 325.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Sb5O14 (mp-779294) | 0.4599 | 0.079 | 3 |
Na2Sb4O11 (mp-774074) | 0.4887 | 0.070 | 3 |
K2Sb4O11 (mp-27140) | 0.5121 | 0.000 | 3 |
K3Sb5O14 (mp-557989) | 0.1935 | 0.018 | 3 |
Rb3Sb5O14 (mp-556234) | 0.3407 | 0.000 | 3 |
LiNb(TeO4)3 (mp-758389) | 0.6583 | 0.013 | 4 |
LiSb(TeO4)3 (mp-849732) | 0.6616 | 0.008 | 4 |
K3BSb4O13 (mp-558607) | 0.5396 | 0.000 | 4 |
GaTeO3F (mp-558984) | 0.6871 | 0.000 | 4 |
LiV(IO4)2 (mp-566833) | 0.6721 | 0.001 | 4 |
Mn7F18 (mp-765911) | 0.7398 | 0.041 | 2 |
W3O8 (mvc-788) | 0.7006 | 0.088 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sb O |
Final Energy/Atom-5.7764 eV |
Corrected Energy-547.6476 eV
-547.6476 eV = -508.3194 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction)
|