Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.637 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
11.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.531 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 77710 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.000 273.4
Ni (mp-23) <1 1 0> <1 1 0> 0.000 191.4
PbS (mp-21276) <1 0 0> <1 0 0> 0.001 180.4
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.012 319.0
MgO (mp-1265) <1 0 0> <1 0 0> 0.012 90.2
Si (mp-149) <1 1 1> <1 1 1> 0.019 156.3
Si (mp-149) <1 1 0> <1 1 0> 0.020 127.6
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.022 156.3
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.023 127.6
GaN (mp-804) <0 0 1> <1 1 1> 0.025 117.2
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.030 293.2
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.030 350.9
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.032 127.6
KCl (mp-23193) <1 0 0> <1 0 0> 0.039 203.0
SiC (mp-11714) <0 0 1> <1 1 1> 0.042 156.3
GaP (mp-2490) <1 1 1> <1 1 1> 0.043 156.3
GaP (mp-2490) <1 1 0> <1 1 0> 0.044 127.6
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.046 225.5
C (mp-66) <1 1 1> <1 1 1> 0.047 156.3
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.048 112.8
SiC (mp-7631) <0 0 1> <1 1 1> 0.048 156.3
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.059 156.3
Te2Mo (mp-602) <1 0 1> <1 1 0> 0.062 223.3
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.063 112.8
CaF2 (mp-2741) <1 1 1> <1 1 1> 0.089 156.3
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.091 127.6
C (mp-48) <1 0 1> <1 1 0> 0.101 159.5
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.104 287.1
MgAl2O4 (mp-3536) <1 1 1> <1 1 1> 0.113 117.2
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.113 203.0
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.116 95.7
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.117 350.9
MgF2 (mp-1249) <1 1 1> <1 1 1> 0.124 273.4
LiF (mp-1138) <1 1 1> <1 1 1> 0.129 117.2
LiF (mp-1138) <1 1 0> <1 1 0> 0.132 95.7
TeO2 (mp-2125) <0 0 1> <1 1 1> 0.136 195.3
Cu (mp-30) <1 1 1> <1 1 1> 0.140 156.3
GaTe (mp-542812) <1 0 0> <1 1 0> 0.173 223.3
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.174 112.8
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.175 157.9
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.190 287.1
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.193 255.2
InP (mp-20351) <1 0 0> <1 0 0> 0.195 180.4
AlN (mp-661) <0 0 1> <1 1 0> 0.195 127.6
LaAlO3 (mp-2920) <1 1 1> <1 1 0> 0.195 127.6
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.197 225.5
PbSe (mp-2201) <1 1 1> <1 1 1> 0.198 273.4
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.214 203.0
LaAlO3 (mp-2920) <0 0 1> <1 1 0> 0.215 127.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.216 287.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
283 51 51 0 0 0
51 283 51 0 0 0
51 51 283 0 0 0
0 0 0 74 0 0
0 0 0 0 74 0
0 0 0 0 0 74
Compliance Tensor Sij (10-12Pa-1)
3.7 -0.6 -0.6 0 0 0
-0.6 3.7 -0.6 0 0 0
-0.6 -0.6 3.7 0 0 0
0 0 0 13.4 0 0
0 0 0 0 13.4 0
0 0 0 0 0 13.4
Shear Modulus GV
91 GPa
Bulk Modulus KV
128 GPa
Shear Modulus GR
87 GPa
Bulk Modulus KR
128 GPa
Shear Modulus GVRH
89 GPa
Bulk Modulus KVRH
128 GPa
Elastic Anisotropy
0.24
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.037 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
ThN (mp-834) 0.0000 0.000 2
ErBi (mp-23245) 0.0000 0.000 2
CaSe (mp-1415) 0.0000 0.000 2
SnAs (mp-2182) 0.0000 0.030 2
ErAs (mp-1688) 0.0000 0.000 2
As (mp-10) 0.0000 0.112 1
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Yb_2 O
Final Energy/Atom
-6.5300 eV
Corrected Energy
-13.7623 eV
-13.7623 eV = -13.0600 eV (uncorrected energy) - 0.7023 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 77710
  • 151764
Submitted by
User remarks:
  • Yttrium(II) oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)