material

Te2O5

ID:

mp-12177

DOI:

10.17188/1188613


Tags: Tellurium tellurium(VI) oxide Tellurium(VI) tellurium(IV) pentaoxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.429 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.29 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.697 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21 [4]
Hall
P 2yb
Point Group
2
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 2523 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.002 132.2
Al2O3 (mp-1143) <1 0 0> <1 0 -1> 0.003 126.2
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.011 132.2
ZrO2 (mp-2858) <1 1 1> <0 1 0> 0.015 307.0
YVO4 (mp-19133) <1 0 1> <1 0 1> 0.016 207.5
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.018 158.7
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.023 238.0
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.024 155.6
NdGaO3 (mp-3196) <1 1 0> <0 1 1> 0.025 307.3
MoS2 (mp-1434) <1 0 1> <1 0 1> 0.026 207.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.029 105.8
CdWO4 (mp-19387) <1 1 0> <1 1 1> 0.030 203.8
SrTiO3 (mp-4651) <1 1 1> <1 0 1> 0.031 207.5
CaF2 (mp-2741) <1 0 0> <0 1 1> 0.031 153.6
BN (mp-984) <1 0 0> <0 1 0> 0.033 307.0
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.034 158.7
YAlO3 (mp-3792) <0 0 1> <0 1 1> 0.034 256.1
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.036 132.2
MgF2 (mp-1249) <1 1 0> <1 1 1> 0.036 203.8
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.036 52.9
MoS2 (mp-1434) <1 1 1> <0 0 1> 0.038 238.0
CdWO4 (mp-19387) <0 0 1> <0 1 1> 0.039 153.6
LiF (mp-1138) <1 1 1> <0 0 1> 0.039 343.8
AlN (mp-661) <1 0 1> <1 1 0> 0.042 176.3
SiC (mp-8062) <1 1 0> <1 0 -1> 0.044 294.6
Si (mp-149) <1 1 0> <0 0 1> 0.044 211.5
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.045 211.5
Ni (mp-23) <1 1 1> <0 1 1> 0.046 256.1
Mg (mp-153) <1 0 1> <1 0 -1> 0.047 168.3
GaP (mp-2490) <1 0 0> <0 1 1> 0.048 153.6
SiC (mp-7631) <1 0 0> <1 1 0> 0.048 235.1
GaTe (mp-542812) <1 0 0> <1 0 1> 0.049 311.3
CsI (mp-614603) <1 0 0> <0 1 1> 0.049 307.3
LiGaO2 (mp-5854) <0 1 0> <0 1 0> 0.051 131.6
NdGaO3 (mp-3196) <0 0 1> <0 1 1> 0.052 153.6
ZnO (mp-2133) <1 1 1> <0 0 1> 0.055 158.7
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.056 293.9
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.056 105.8
MoS2 (mp-1434) <1 1 0> <0 0 1> 0.064 238.0
Ag (mp-124) <1 1 0> <1 0 0> 0.064 195.7
ZnO (mp-2133) <0 0 1> <1 0 0> 0.065 234.8
Te2W (mp-22693) <1 0 0> <1 1 0> 0.066 293.9
CsI (mp-614603) <1 1 1> <0 0 1> 0.070 105.8
WS2 (mp-224) <1 1 0> <0 0 1> 0.072 79.3
Au (mp-81) <1 1 0> <1 0 0> 0.072 195.7
MoSe2 (mp-1634) <1 0 1> <0 1 0> 0.073 263.1
GaN (mp-804) <1 0 1> <1 0 -1> 0.075 168.3
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.076 132.2
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.076 203.8
SrTiO3 (mp-4651) <0 0 1> <0 1 1> 0.077 153.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
71 9 9 0 14 0
9 108 59 0 8 0
9 59 161 0 11 0
0 0 0 95 0 12
14 8 11 0 21 0
0 0 0 12 0 28
Compliance Tensor Sij (10-12Pa-1)
16.3 -0.5 0 0 -10.4 0
-0.5 11.6 -4.1 0 -1.9 0
0 -4.1 7.9 0 -2.7 0
0 0 0 11.1 0 -5
-10.4 -1.9 -2.7 0 56.7 0
0 0 0 -5 0 38.6
Shear Modulus GV
46 GPa
Bulk Modulus KV
55 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
38 GPa
Shear Modulus GVRH
39 GPa
Bulk Modulus KVRH
46 GPa
Elastic Anisotropy
2.88
Poisson's Ratio
0.17

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.01829 0.00000 0.97792
1.18261 0.19808 -0.23703 0.00000 0.24717 0.00000
0.00000 0.00000 0.00000 -0.03208 0.00000 0.11376
Piezoelectric Modulus ‖eijmax
1.24703 C/m2
Crystallographic Direction vmax
0.00000
9.00000
-1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.21 0.00 0.77
0.00 5.01 0.00
0.77 0.00 4.63
Dielectric Tensor εij (total)
18.38 0.00 5.31
0.00 16.56 0.00
5.31 0.00 13.04
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.95
Polycrystalline dielectric constant εpoly
(total)
15.99
Refractive Index n
2.23
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMnF5 (mp-766918) 0.6603 0.019 3
LiFeF5 (mp-776770) 0.6055 0.238 3
ZnWF5 (mvc-3753) 0.6608 0.000 3
LiMnF5 (mp-767597) 0.5924 0.169 3
Tl3(SbO3)8 (mp-752438) 0.6537 0.084 3
AgF3 (mp-18536) 0.7452 0.000 2
Cr2F5 (mp-558380) 0.7246 0.003 2
Te4O9 (mp-27127) 0.4164 0.001 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Te O
Final Energy/Atom
-5.3595 eV
Corrected Energy
-82.0559 eV
-82.0559 eV = -75.0330 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 2523
  • 191342
Submitted by
User remarks:
  • Tellurium tellurium(VI) oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)