material

Ba

ID:

mp-122

DOI:

10.17188/1188649


Tags: Barium - bcc Barium

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.58 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Im3m [229]
Hall
-I 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 44719 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.000 43.8
LiNbO3 (mp-3731) <0 0 1> <1 1 1> 0.000 306.8
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 0 0> 0.000 227.7
KP(HO2)2 (mp-23959) <0 1 1> <1 1 0> 0.001 107.4
C (mp-66) <1 1 1> <1 0 0> 0.005 177.1
LiTaO3 (mp-3666) <0 0 1> <1 1 1> 0.005 306.8
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.005 177.1
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.007 126.5
Au (mp-81) <1 0 0> <1 0 0> 0.009 227.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.009 126.5
InSb (mp-20012) <1 1 1> <1 1 1> 0.010 306.8
InAs (mp-20305) <1 1 0> <1 1 0> 0.010 107.4
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.014 107.4
CdTe (mp-406) <1 1 1> <1 1 1> 0.014 306.8
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.017 227.7
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.018 143.1
C (mp-66) <1 0 0> <1 0 0> 0.019 25.3
SiC (mp-11714) <0 0 1> <1 1 1> 0.019 131.5
KCl (mp-23193) <1 0 0> <1 0 0> 0.020 202.4
SiC (mp-7631) <0 0 1> <1 1 1> 0.022 131.5
C (mp-66) <1 1 0> <1 1 0> 0.023 35.8
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.026 286.3
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.026 151.8
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.026 329.0
SiC (mp-8062) <1 1 0> <1 1 0> 0.026 107.4
Ag (mp-124) <1 0 0> <1 0 0> 0.027 227.7
SiC (mp-8062) <1 1 1> <1 1 1> 0.028 131.5
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.029 219.1
LiF (mp-1138) <1 1 0> <1 1 0> 0.031 71.6
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.031 126.5
BN (mp-984) <0 0 1> <1 0 0> 0.034 177.1
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.039 175.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.042 126.5
WS2 (mp-224) <1 0 1> <1 0 0> 0.042 227.7
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.043 286.3
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.044 278.3
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.044 177.1
MoSe2 (mp-1634) <0 0 1> <1 1 0> 0.049 143.1
WSe2 (mp-1821) <0 0 1> <1 1 0> 0.049 143.1
CaCO3 (mp-3953) <1 0 1> <1 0 0> 0.049 177.1
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.050 126.5
Al (mp-134) <1 1 1> <1 1 0> 0.053 143.1
Ge (mp-32) <1 1 0> <1 1 0> 0.056 143.1
AlN (mp-661) <0 0 1> <1 1 1> 0.058 175.3
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.058 286.3
Ge (mp-32) <1 1 1> <1 1 1> 0.060 175.3
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.060 227.7
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.061 263.0
GaSe (mp-1943) <0 0 1> <1 1 0> 0.063 250.5
CdSe (mp-2691) <1 1 0> <1 1 0> 0.066 107.4
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
0.31 J/m2 (0.02 eV/Å2)
Weighted work function Φ
2.33 eV
Shape factor η
5.15
Surface energy anisotropy αγ
0.014
Miller Indices
(hkl)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(110) 0.31, 0.02 2.35 0.75
(100) 0.32, 0.02 2.28 0.23
(320) 0.33, 0.02 2.30 0.03
(210) 0.34, 0.02 1.90 0.00
(310) 0.35, 0.02 2.25 0.00
(331) 0.36, 0.02 2.35 0.00
(321) 0.36, 0.02 2.04 0.00
(311) 0.37, 0.02 2.21 0.00
(211) 0.37, 0.02 2.30 0.00
(221) 0.37, 0.02 2.20 0.00
(322) 0.38, 0.02 2.31 0.00
(332) 0.38, 0.02 2.31 0.00
(111) 0.39, 0.02 2.24 0.00

Grain Boundaries

Reference for grain boundary energies and properties:
Sigma, Σ
type
rotation axis rotation angle GB plane Energy, 𝛾GB
(J/m2)
Work of Separation, Wsep
(J/m2)
Structure
(CIF)
3 tilt [110] 109.47 (112) 0.03 0.72
3 tilt [111] 180.00 (110) 0.04 0.58
3 twist [111] 60.00 (111) 0.18 0.59
5 tilt [100] 36.87 (012) 0.14 0.54
5 tilt [100] 53.13 (013) 0.16 0.53
5 twist [100] 36.87 (100) 0.28 0.36
7 tilt [111] 38.21 (132) 0.14 0.58
7 twist [111] 38.21 (111) 0.25 0.52
9 twist [110] 38.94 (110) 0.10 0.53
9 tilt [110] 38.94 (221) 0.19 0.56

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
12 7 7 0 0 0
7 12 7 0 0 0
7 7 12 0 0 0
0 0 0 10 0 0
0 0 0 0 10 0
0 0 0 0 0 10
Compliance Tensor Sij (10-12Pa-1)
153.6 -58 -58 0 0 0
-58 153.6 -58 0 0 0
-58 -58 153.6 0 0 0
0 0 0 98.2 0 0
0 0 0 0 98.2 0
0 0 0 0 0 98.2
Shear Modulus GV
7 GPa
Bulk Modulus KV
9 GPa
Shear Modulus GR
4 GPa
Bulk Modulus KR
9 GPa
Shear Modulus GVRH
6 GPa
Bulk Modulus KVRH
9 GPa
Elastic Anisotropy
3.05
Poisson's Ratio
0.23

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -1.923 63.601 0.492 1.831
pack_evans_james -1.923 63.600 0.055 1.948
vinet -1.923 63.592 0.495 2.940
tait -1.923 63.575 0.055 4.021
birch_euler -1.923 63.578 0.062 -0.998
pourier_tarantola -1.923 63.595 0.009 0.953
birch_lagrange -1.924 63.612 0.033 4.816
murnaghan -1.923 63.624 0.054 1.897
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ScInAu2 (mp-30395) 0.0000 0.000 3
TbInAg2 (mp-22382) 0.0000 0.000 3
Li2HgGe (mp-16341) 0.0000 0.052 3
Li2SnGe (mp-12094) 0.0000 0.149 3
Li2InPd (mp-21029) 0.0000 0.000 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
TiFeCoGe (mp-1018012) 0.0000 0.028 4
LiMgSbPd (mp-10179) 0.0000 0.090 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
Rb3Bi (mp-23304) 0.0000 0.028 2
Sr3In (mp-31349) 0.0000 0.131 2
Fe3Ge (mp-20711) 0.0000 0.000 2
Li3Sb (mp-2074) 0.0000 0.000 2
NaTl (mp-1564) 0.0000 0.000 2
Eu (mp-20071) 0.0000 0.083 1
Ce (mp-10024) 0.0000 0.228 1
Lu (mp-10190) 0.0000 0.132 1
Np (mp-10207) 0.0000 0.447 1
Gd (mp-11421) 0.0000 0.088 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv
Final Energy/Atom
-1.9190 eV
Corrected Energy
-1.9190 eV
Uncorrected energy = -1.9190 eV Corrected energy = -1.9190 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 108091
  • 76156
  • 615774
  • 94258
  • 191758
  • 426927
  • 44719
  • 56132
  • 77367
Submitted by
User remarks:
  • Barium