material

SrCN2

ID:

mp-12317

DOI:

10.17188/1188698


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.050 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.261 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <0 0 1> 0.000 166.9
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.000 125.2
InAs (mp-20305) <1 1 1> <0 0 1> 0.001 264.2
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.003 264.2
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.004 166.9
WS2 (mp-224) <0 0 1> <0 0 1> 0.004 166.9
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.005 264.2
SiC (mp-7631) <1 1 0> <1 0 0> 0.005 243.4
GaN (mp-804) <1 0 0> <1 0 0> 0.006 304.2
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.006 125.2
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.006 125.2
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.007 180.8
C (mp-66) <1 1 1> <0 0 1> 0.008 264.2
LaF3 (mp-905) <0 0 1> <0 0 1> 0.012 180.8
TePb (mp-19717) <1 1 1> <0 0 1> 0.014 222.5
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.014 222.5
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.018 125.2
NaCl (mp-22862) <1 1 1> <0 0 1> 0.023 55.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.025 264.2
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.030 180.8
SiC (mp-11714) <1 0 0> <0 0 1> 0.030 347.7
MgO (mp-1265) <1 0 0> <0 0 1> 0.031 292.1
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.033 111.3
SiC (mp-7631) <1 1 1> <1 0 0> 0.035 243.4
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.036 333.8
Mg (mp-153) <1 1 0> <0 0 1> 0.040 292.1
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.041 264.2
CdSe (mp-2691) <1 1 1> <0 0 1> 0.045 264.2
BN (mp-984) <1 0 0> <0 0 1> 0.052 250.3
Ni (mp-23) <1 0 0> <0 0 1> 0.055 97.4
Ni (mp-23) <1 1 0> <0 0 1> 0.058 69.5
GaSb (mp-1156) <1 1 1> <0 0 1> 0.061 264.2
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.062 304.2
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.063 83.4
PbS (mp-21276) <1 0 0> <0 0 1> 0.065 292.1
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.070 222.5
GaN (mp-804) <1 1 0> <0 0 1> 0.072 292.1
BN (mp-984) <0 0 1> <0 0 1> 0.074 166.9
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.079 180.8
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.081 97.4
LiF (mp-1138) <1 1 1> <0 0 1> 0.082 264.2
PbSe (mp-2201) <1 1 1> <0 0 1> 0.085 264.2
CdS (mp-672) <1 1 0> <0 0 1> 0.086 250.3
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.086 182.5
GaSe (mp-1943) <0 0 1> <0 0 1> 0.088 166.9
BN (mp-984) <1 1 1> <0 0 1> 0.088 306.0
AlN (mp-661) <1 1 0> <1 0 0> 0.089 243.4
CdS (mp-672) <0 0 1> <0 0 1> 0.090 180.8
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.091 312.1
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.096 304.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
81 31 43 -4 0 0
31 81 43 4 0 0
43 43 139 0 0 0
-4 4 0 8 0 0
0 0 0 0 8 -4
0 0 0 0 -4 25
Compliance Tensor Sij (10-12Pa-1)
16.5 -4.8 -3.6 9.8 0 0
-4.8 16.5 -3.6 -9.8 0 0
-3.6 -3.6 9.5 0 0 0
9.8 -9.8 0 136.9 0 0
0 0 0 0 136.9 19.5
0 0 0 0 19.5 42.7
Shear Modulus GV
20 GPa
Bulk Modulus KV
60 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
55 GPa
Shear Modulus GVRH
17 GPa
Bulk Modulus KVRH
57 GPa
Elastic Anisotropy
3.03
Poisson's Ratio
0.37

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.61 0.00 0.00
0.00 2.61 0.00
0.00 0.00 4.24
Dielectric Tensor εij (total)
6.81 0.00 0.00
0.00 6.81 0.00
0.00 0.00 10.25
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.15
Polycrystalline dielectric constant εpoly
(total)
7.96
Refractive Index n
1.77
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BaCN2 (mp-1029375) 0.1543 0.000 3
YHO2 (mp-768231) 0.1951 0.082 3
CaCN2 (mp-4124) 0.1386 0.000 3
CdCN2 (mp-10969) 0.1607 0.000 3
NaHF2 (mp-27837) 0.0946 0.000 3
KC2IN2 (mp-567299) 0.5925 0.473 4
NaCNO (mp-546500) 0.3144 0.000 4
NaAg(CN)2 (mp-568422) 0.4681 0.217 4
KAg(CN)2 (mp-582994) 0.5537 0.191 4
KAu(CN)2 (mp-672348) 0.5119 0.117 4
NaN3 (mp-22003) 0.3729 0.000 2
NaN3 (mp-570538) 0.4375 0.000 2
NaN3 (mp-1066400) 0.2021 0.002 2
NaN3 (mp-1064952) 0.4121 0.001 2
LiN3 (mp-2659) 0.4241 0.000 2
Sr2LiCBr3N2 (mp-569782) 0.7030 0.000 5
LiEu2CBr3N2 (mp-568863) 0.7034 0.000 5
K2NaAg3(CN)6 (mp-6855) 0.6743 0.207 5
AgSbH2C2(NF3)2 (mp-690698) 0.7350 0.161 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv C N
Final Energy/Atom
-7.7553 eV
Corrected Energy
-31.0213 eV
-31.0213 eV = -31.0213 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)