Final Magnetic Moment0.019 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.749 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHo + HoPd |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 301.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 301.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 216.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 216.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 245.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 275.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 173.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 336.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 214.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 259.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 60.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 214.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 203.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 303.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 367.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 216.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 245.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 153.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 181.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 245.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 129.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 275.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 153.1 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 173.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 181.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 216.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 91.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 60.4 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 270.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 275.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 129.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 91.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 275.7 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 216.6 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 222.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 346.5 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 346.5 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 259.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 275.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 336.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 270.8 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 297.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 259.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 214.4 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 173.3 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 270.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 275.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 259.9 |
Al (mp-134) | <1 0 0> | <1 1 0> | 129.9 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 216.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
U2InNi2 (mp-647194) | 0.1522 | 0.183 | 3 |
Pu2InRh2 (mp-640039) | 0.1943 | 0.000 | 3 |
Np2InNi2 (mp-20091) | 0.2354 | 0.110 | 3 |
Tb2MgPd2 (mp-16652) | 0.1647 | 0.008 | 3 |
Yb2CdPd2 (mp-4663) | 0.1905 | 0.000 | 3 |
Yb3Ag2 (mp-571608) | 0.1076 | 0.000 | 2 |
Dy3Pd2 (mp-12543) | 0.0446 | 0.000 | 2 |
Er3Pd2 (mp-12545) | 0.0584 | 0.000 | 2 |
Si2W3 (mp-1079377) | 0.1969 | 0.210 | 2 |
Gd3Pd2 (mp-22077) | 0.1134 | 0.014 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Pd |
Final Energy/Atom-5.5692 eV |
Corrected Energy-55.6921 eV
-55.6921 eV = -55.6921 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)