material

LiMgAs

ID:

mp-12558

DOI:

10.17188/1188977


Tags: Lithium magnesium arsenide

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.744 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 107954 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 0 0> <1 0 0> 0.000 308.8
CdSe (mp-2691) <1 0 0> <1 0 0> 0.000 38.6
CdSe (mp-2691) <1 1 0> <1 1 0> 0.000 54.6
CdSe (mp-2691) <1 1 1> <1 1 1> 0.000 66.9
BN (mp-984) <0 0 1> <1 1 1> 0.001 267.5
GaSb (mp-1156) <1 0 0> <1 0 0> 0.001 38.6
GaSb (mp-1156) <1 1 0> <1 1 0> 0.001 54.6
GaSb (mp-1156) <1 1 1> <1 1 1> 0.001 66.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.003 308.8
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.004 66.9
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.005 66.9
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.005 154.4
PbSe (mp-2201) <1 0 0> <1 0 0> 0.007 38.6
PbSe (mp-2201) <1 1 0> <1 1 0> 0.007 54.6
PbSe (mp-2201) <1 1 1> <1 1 1> 0.007 66.9
SiC (mp-7631) <1 1 0> <1 1 0> 0.014 163.8
SiC (mp-8062) <1 0 0> <1 0 0> 0.015 38.6
SiC (mp-8062) <1 1 0> <1 1 0> 0.015 54.6
GaSe (mp-1943) <0 0 1> <1 1 1> 0.017 200.6
CdS (mp-672) <0 0 1> <1 1 1> 0.018 200.6
C (mp-66) <1 1 0> <1 1 0> 0.018 54.6
C (mp-66) <1 1 1> <1 1 1> 0.018 66.9
TePb (mp-19717) <1 0 0> <1 0 0> 0.019 347.5
LiF (mp-1138) <1 1 1> <1 1 1> 0.022 200.6
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.023 218.4
WS2 (mp-224) <0 0 1> <1 0 0> 0.025 308.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.025 308.8
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.025 66.9
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.027 308.8
Ag (mp-124) <1 0 0> <1 0 0> 0.029 154.4
AlN (mp-661) <0 0 1> <1 0 0> 0.029 270.2
Ag (mp-124) <1 1 0> <1 1 0> 0.029 218.4
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.029 193.0
Ag (mp-124) <1 1 1> <1 1 1> 0.029 267.5
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.031 38.6
ZnTe (mp-2176) <1 1 0> <1 1 0> 0.031 54.6
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.031 66.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.032 115.8
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.033 163.8
Mg (mp-153) <0 0 1> <1 0 0> 0.034 308.8
InAs (mp-20305) <1 0 0> <1 0 0> 0.038 38.6
Cu (mp-30) <1 0 0> <1 1 0> 0.038 273.0
InAs (mp-20305) <1 1 0> <1 1 0> 0.039 54.6
InAs (mp-20305) <1 1 1> <1 1 1> 0.039 66.9
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.040 308.8
SiC (mp-7631) <1 0 1> <1 0 0> 0.048 193.0
CdTe (mp-406) <1 0 0> <1 0 0> 0.051 347.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.062 347.5
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.066 193.0
Au (mp-81) <1 0 0> <1 0 0> 0.072 154.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
93 23 23 0 0 0
23 93 23 0 0 0
23 23 93 0 0 0
0 0 0 38 0 0
0 0 0 0 38 0
0 0 0 0 0 38
Compliance Tensor Sij (10-12Pa-1)
11.9 -2.4 -2.4 0 0 0
-2.4 11.9 -2.4 0 0 0
-2.4 -2.4 11.9 0 0 0
0 0 0 26.5 0 0
0 0 0 0 26.5 0
0 0 0 0 0 26.5
Shear Modulus GV
37 GPa
Bulk Modulus KV
47 GPa
Shear Modulus GR
37 GPa
Bulk Modulus KR
47 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
47 GPa
Elastic Anisotropy
0.01
Poisson's Ratio
0.19

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NbCoSb (mp-31460) 0.0000 0.021 3
TiFeSb (mp-10755) 0.0000 0.000 3
LiGaSi (mp-11390) 0.0000 0.071 3
SmSnAu (mp-13305) 0.0000 0.000 3
YbCuGe (mp-13306) 0.0000 0.162 3
TiF2 (mp-282) 0.0000 0.248 2
SnO2 (mp-12979) 0.0000 0.246 2
Na2Se (mp-1266) 0.0000 0.000 2
Rb2Se (mp-11327) 0.0000 0.000 2
H2Se (mp-24420) 0.0000 0.645 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Mg_pv As
Final Energy/Atom
-3.4673 eV
Corrected Energy
-10.4018 eV
Uncorrected energy = -10.4018 eV Corrected energy = -10.4018 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 107954
Submitted by
User remarks:
  • Lithium magnesium arsenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)