Final Magnetic Moment4.179 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.241 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAsPd3 + MnAs + Mn3Pd5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 224.3 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 277.5 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 198.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 68.7 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 68.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 198.2 |
C (mp-48) | <0 0 1> | <1 1 1> | 68.7 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 356.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 317.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 317.1 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 198.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 39.6 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 198.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 56.1 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 68.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 317.1 |
WS2 (mp-224) | <0 0 1> | <1 1 1> | 274.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 158.6 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 274.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 168.2 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 198.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 206.0 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 356.8 |
Si (mp-149) | <1 1 0> | <1 1 0> | 168.2 |
Si (mp-149) | <1 1 1> | <1 1 1> | 206.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 274.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 317.1 |
C (mp-66) | <1 0 0> | <1 0 0> | 317.1 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 158.6 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 274.6 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 274.6 |
TiO2 (mp-2657) | <1 1 1> | <1 1 1> | 206.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 79.3 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 277.5 |
C (mp-48) | <1 0 1> | <1 1 0> | 336.4 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 56.1 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 68.7 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 1> | 274.6 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 168.2 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 280.3 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 168.2 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 168.2 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 274.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 317.1 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 198.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 1> | 274.6 |
Au (mp-81) | <1 0 0> | <1 0 0> | 158.6 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 198.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 224.3 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 356.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
129 | 131 | 131 | 0 | 0 | 0 |
131 | 129 | 131 | 0 | 0 | 0 |
131 | 131 | 129 | 0 | 0 | 0 |
0 | 0 | 0 | 45 | 0 | 0 |
0 | 0 | 0 | 0 | 45 | 0 |
0 | 0 | 0 | 0 | 0 | 45 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-462.3 | 232.4 | 232.4 | 0 | 0 | 0 |
232.4 | -462.3 | 232.4 | 0 | 0 | 0 |
232.4 | 232.4 | -462.3 | 0 | 0 | 0 |
0 | 0 | 0 | 22.4 | 0 | 0 |
0 | 0 | 0 | 0 | 22.4 | 0 |
0 | 0 | 0 | 0 | 0 | 22.4 |
Shear Modulus GV27 GPa |
Bulk Modulus KV130 GPa |
Shear Modulus GR-2 GPa |
Bulk Modulus KR130 GPa |
Shear Modulus GVRH12 GPa |
Bulk Modulus KVRH130 GPa |
Elastic Anisotropy-77.00 |
Poisson's Ratio0.45 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiAlNi2 (mp-7187) | 0.0000 | 0.000 | 3 |
ScInPt2 (mp-20521) | 0.0000 | 0.000 | 3 |
TbSnPd2 (mp-5385) | 0.0000 | 0.000 | 3 |
InFeCo2 (mp-21211) | 0.0000 | 0.103 | 3 |
NbAlNi2 (mp-4813) | 0.0000 | 0.007 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Mn3Si (mp-20211) | 0.0000 | 0.000 | 2 |
NdMg3 (mp-1787) | 0.0000 | 0.000 | 2 |
PrMg3 (mp-428) | 0.0000 | 0.000 | 2 |
AlFe3 (mp-2018) | 0.0000 | 0.002 | 2 |
K3Sb (mp-10159) | 0.0000 | 0.028 | 2 |
Sr (mp-95) | 0.0000 | 0.013 | 1 |
Yb (mp-71) | 0.0000 | 0.017 | 1 |
Fe (mp-13) | 0.0000 | 0.000 | 1 |
Nb (mp-75) | 0.0000 | 0.000 | 1 |
Li (mp-135) | 0.0000 | 0.005 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv As Pd |
Final Energy/Atom-6.2864 eV |
Corrected Energy-25.1454 eV
-25.1454 eV = -25.1454 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)