Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.107 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrPt |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 72.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 304.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 217.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 218.2 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 72.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 217.6 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 133.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 266.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 252.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 290.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 201.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 174.1 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 72.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 217.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 188.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 94.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 321.9 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 236.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 109.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 90.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 345.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 217.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 254.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 345.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 345.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 290.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 235.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 327.3 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 214.6 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 181.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 66.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 333.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 218.2 |
BN (mp-984) | <1 0 0> | <0 1 1> | 94.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 200.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 174.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 174.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 217.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 145.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 217.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 200.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 94.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 261.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 94.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 321.9 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 236.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 235.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 174.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 145.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 217.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.7353 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.7304 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.7461 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.6953 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.3953 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.6662 | 0.106 | 4 |
YbPt (mp-570180) | 0.1531 | 0.019 | 2 |
NdPt (mp-570934) | 0.0584 | 0.006 | 2 |
LaPd (mp-1002115) | 0.1160 | 0.000 | 2 |
PrPd (mp-999291) | 0.1607 | 0.000 | 2 |
LaPt (mp-1002104) | 0.1368 | 0.000 | 2 |
Si (mp-1001113) | 0.5363 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Pt |
Final Energy/Atom-6.5325 eV |
Corrected Energy-26.1299 eV
-26.1299 eV = -26.1299 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)