material

BaPdF4

ID:

mp-12623

DOI:

10.17188/1189089


Tags: Barium palladium fluoride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.873 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.87 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.433 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 108991 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.000 157.8
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.000 39.5
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.001 355.1
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.007 315.6
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.009 197.3
Cu (mp-30) <1 1 0> <0 0 1> 0.011 276.2
AlN (mp-661) <1 0 1> <0 0 1> 0.014 355.1
ZnO (mp-2133) <1 0 1> <1 0 0> 0.015 138.9
Au (mp-81) <1 0 0> <0 0 1> 0.020 157.8
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.020 315.6
PbSe (mp-2201) <1 1 0> <0 0 1> 0.021 276.2
GaN (mp-804) <0 0 1> <0 0 1> 0.025 315.6
InSb (mp-20012) <1 0 0> <0 0 1> 0.025 355.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.028 276.2
AlN (mp-661) <0 0 1> <1 0 1> 0.030 239.6
CdTe (mp-406) <1 0 0> <0 0 1> 0.032 355.1
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.034 355.1
GaSb (mp-1156) <1 1 0> <0 0 1> 0.035 276.2
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.037 138.9
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.037 138.9
CdS (mp-672) <0 0 1> <1 0 0> 0.042 138.9
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.042 276.2
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.042 294.6
InP (mp-20351) <1 0 0> <0 0 1> 0.045 315.6
C (mp-66) <1 0 0> <0 0 1> 0.047 315.6
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.048 315.6
CdSe (mp-2691) <1 1 0> <0 0 1> 0.049 276.2
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.049 208.3
Te2W (mp-22693) <1 0 0> <0 0 1> 0.050 197.3
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.053 197.3
Ag (mp-124) <1 0 0> <0 0 1> 0.054 157.8
Mg (mp-153) <0 0 1> <1 0 0> 0.056 69.4
Ni (mp-23) <1 0 0> <0 0 1> 0.061 157.8
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.063 315.6
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.064 197.3
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.068 208.3
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.071 78.9
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.072 276.2
MoS2 (mp-1434) <1 0 1> <0 0 1> 0.073 276.2
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.073 208.3
WS2 (mp-224) <0 0 1> <0 0 1> 0.074 355.1
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.074 355.1
LaF3 (mp-905) <1 1 0> <1 0 0> 0.083 277.8
YVO4 (mp-19133) <1 1 0> <0 0 1> 0.088 197.3
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.090 315.6
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.091 196.4
Te2W (mp-22693) <1 0 1> <0 0 1> 0.091 197.3
SiC (mp-11714) <0 0 1> <0 0 1> 0.092 197.3
GaN (mp-804) <1 1 0> <1 1 0> 0.092 294.6
Mg (mp-153) <1 0 0> <0 0 1> 0.095 197.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
65 50 43 0 0 0
50 65 43 0 0 0
43 43 80 0 0 0
0 0 0 16 0 0
0 0 0 0 16 0
0 0 0 0 0 23
Compliance Tensor Sij (10-12Pa-1)
40.8 -26.2 -7.8 0 0 0
-26.2 40.8 -7.8 0 0 0
-7.8 -7.8 20.7 0 0 0
0 0 0 61.9 0 0
0 0 0 0 61.9 0
0 0 0 0 0 43.1
Shear Modulus GV
16 GPa
Bulk Modulus KV
53 GPa
Shear Modulus GR
14 GPa
Bulk Modulus KR
53 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
53 GPa
Elastic Anisotropy
0.76
Poisson's Ratio
0.37

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.67 0.00 -0.00
0.00 2.67 0.00
-0.00 0.00 2.83
Dielectric Tensor εij (total)
6.47 0.00 -0.00
0.00 6.47 0.00
-0.00 0.00 6.75
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.72
Polycrystalline dielectric constant εpoly
(total)
6.56
Refractive Index n
1.65
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaAuF4 (mp-7388) 0.2521 0.000 3
KAuF4 (mp-5309) 0.2380 0.000 3
PdPbF4 (mp-20805) 0.1991 0.000 3
SrCuF4 (mp-12265) 0.2320 0.000 3
SrPdF4 (mp-12622) 0.2085 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Pd F
Final Energy/Atom
-5.0028 eV
Corrected Energy
-63.7301 eV
Uncorrected energy = -60.0341 eV Composition-based energy adjustment (-0.462 eV/atom x 8.0 atoms) = -3.6960 eV Corrected energy = -63.7301 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 108991
Submitted by
User remarks:
  • Barium palladium fluoride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)