Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.479 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/m [176] |
Hall-P 6c |
Point Group6/m |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 230.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 285.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 230.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 230.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 171.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 329.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 296.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 230.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 131.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 263.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 98.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 242.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 80.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 362.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 230.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 263.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 296.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 285.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 285.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 161.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 161.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 285.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 98.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 285.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 65.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 164.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 242.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 197.7 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 171.2 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 262.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 285.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 98.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 296.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 65.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 263.6 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 57.1 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 171.2 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 285.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 98.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 296.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 263.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 242.8 |
BN (mp-984) | <0 0 1> | <1 1 0> | 114.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 230.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 362.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 230.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 296.6 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 296.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 242.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 296.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb3SnS6 (mp-9407) | 0.6605 | 0.000 | 3 |
Ta3SnS6 (mp-9132) | 0.6681 | 0.000 | 3 |
Nb3Te3As (mp-28968) | 0.6070 | 0.000 | 3 |
Hf5ZrTe8 (mp-678358) | 0.2082 | 0.000 | 3 |
LiScI3 (mp-28835) | 0.6414 | 0.048 | 3 |
Nb3Te4 (mp-7564) | 0.5096 | 0.000 | 2 |
Ti3Se4 (mp-9227) | 0.5260 | 0.000 | 2 |
Nb3Se4 (mp-561) | 0.3479 | 0.000 | 2 |
V3S4 (mp-799) | 0.1605 | 0.000 | 2 |
CeSe2 (mp-1080314) | 0.5266 | 0.295 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv S |
Final Energy/Atom-7.7928 eV |
Corrected Energy-114.4066 eV
-114.4066 eV = -109.0990 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)