material

TiAu4

ID:

mp-12635

DOI:

10.17188/1189098


Tags: Titanium auride (1/4) Gold titanium (4/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.279 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
15.87 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/m [87]
Hall
-I 4
Point Group
4/m
Crystal System
tetragonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 0 0> <0 0 1> 0.001 348.6
GaSb (mp-1156) <1 0 0> <0 0 1> 0.002 348.6
Au (mp-81) <1 0 0> <0 0 1> 0.002 87.2
C (mp-66) <1 0 0> <0 0 1> 0.007 217.9
CdSe (mp-2691) <1 0 0> <0 0 1> 0.010 348.6
ZnO (mp-2133) <1 0 1> <1 0 0> 0.011 79.5
AlN (mp-661) <1 1 0> <1 1 0> 0.012 299.8
Te2Mo (mp-602) <0 0 1> <1 1 0> 0.014 262.3
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.015 217.9
CdTe (mp-406) <1 1 0> <1 0 0> 0.024 185.5
Si (mp-149) <1 1 0> <1 0 1> 0.027 255.0
CeO2 (mp-20194) <1 1 0> <1 0 1> 0.031 255.0
SiC (mp-11714) <1 0 0> <1 1 0> 0.033 187.4
InSb (mp-20012) <1 1 0> <1 0 0> 0.036 185.5
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.036 262.3
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.037 217.9
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.037 43.6
Ag (mp-124) <1 0 0> <0 0 1> 0.038 87.2
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.042 153.0
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.043 153.0
CdTe (mp-406) <1 0 0> <0 0 1> 0.057 43.6
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.064 132.5
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.070 79.5
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.072 318.0
SiC (mp-8062) <1 0 0> <0 0 1> 0.074 174.3
InSb (mp-20012) <1 0 0> <0 0 1> 0.076 43.6
Fe2O3 (mp-24972) <0 0 1> <1 1 0> 0.076 299.8
GaP (mp-2490) <1 1 0> <1 0 1> 0.085 255.0
C (mp-48) <1 0 0> <1 0 1> 0.086 153.0
NdGaO3 (mp-3196) <1 1 0> <1 0 1> 0.087 306.0
TePb (mp-19717) <1 0 0> <0 0 1> 0.089 43.6
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.090 255.0
CdWO4 (mp-19387) <0 1 0> <1 1 0> 0.090 262.3
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.095 212.0
GaSe (mp-1943) <1 1 1> <1 0 0> 0.098 238.5
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.102 43.6
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.105 305.0
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.106 57.5
Ga2O3 (mp-886) <1 0 -1> <1 1 1> 0.107 114.9
Mg (mp-153) <1 0 0> <1 0 0> 0.109 132.5
SiC (mp-11714) <0 0 1> <1 1 0> 0.110 262.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.111 318.0
ZnO (mp-2133) <0 0 1> <1 0 0> 0.114 185.5
SiC (mp-7631) <0 0 1> <1 1 0> 0.121 262.3
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.124 348.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.134 217.9
GaSe (mp-1943) <0 0 1> <1 0 1> 0.137 51.0
InAs (mp-20305) <1 0 0> <0 0 1> 0.146 348.6
SiC (mp-8062) <1 1 1> <1 1 0> 0.148 262.3
TePb (mp-19717) <1 1 0> <1 0 0> 0.162 185.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
167 135 135 0 0 0
135 182 112 -0 0 0
135 112 182 0 0 0
0 -0 0 43 0 0
0 0 0 0 66 0
0 0 0 0 0 66
Compliance Tensor Sij (10-12Pa-1)
23.4 -10.8 -10.8 0 0 0
-10.8 13.8 -0.5 0.1 0 0
-10.8 -0.5 13.8 -0.1 0 0
0 0.1 -0.1 23.2 0 0
0 0 0 0 15.1 0
0 0 0 0 0 15.1
Shear Modulus GV
45 GPa
Bulk Modulus KV
144 GPa
Shear Modulus GR
33 GPa
Bulk Modulus KR
144 GPa
Shear Modulus GVRH
39 GPa
Bulk Modulus KVRH
144 GPa
Elastic Anisotropy
1.78
Poisson's Ratio
0.38

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo17 (mp-766895) 0.1988 0.027 3
NaMg6Zr (mp-1022488) 0.2163 0.100 3
Cr8Ni50Mo15W2 (mp-767372) 0.2866 0.028 4
CrFeCoNi (mp-1012640) 0.2964 0.065 4
CrFeCoNi (mp-1096923) 0.2358 0.193 4
Cu4Pd (mp-30594) 0.1308 0.014 2
Mg41Al67 (mp-568106) 0.1965 0.092 2
TaNi3 (mp-569776) 0.1950 0.002 2
MnAu4 (mp-12565) 0.1773 0.000 2
Mg2Si (mp-1074637) 0.1773 0.209 2
Hg (mp-569360) 0.3183 0.001 1
Pr (mp-567630) 0.3042 0.008 1
Sc (mp-1055932) 0.3070 0.052 1
Pr (mp-1059528) 0.2650 0.010 1
Sn (mp-623511) 0.3242 0.061 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Au
Final Energy/Atom
-4.4772 eV
Corrected Energy
-22.3860 eV
-22.3860 eV = -22.3860 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 109132
  • 612411
Submitted by
User remarks:
  • Gold titanium (4/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)