material

CdAu3

ID:

mp-1264

DOI:

10.17188/1189101


Tags: Gold cadmium (3/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.130 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
15.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58414 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 0 0> <1 0 0> 0.000 160.0
CdS (mp-672) <1 0 1> <1 0 0> 0.001 195.5
InP (mp-20351) <1 0 0> <1 0 0> 0.002 35.5
InP (mp-20351) <1 1 0> <1 1 0> 0.002 50.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.007 319.9
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.010 226.2
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.022 150.8
NaCl (mp-22862) <1 1 0> <1 1 0> 0.025 276.5
ZnO (mp-2133) <1 1 1> <1 0 0> 0.027 284.4
Mg (mp-153) <0 0 1> <1 1 0> 0.028 176.0
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.033 71.1
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.035 176.0
WS2 (mp-224) <0 0 1> <1 1 0> 0.035 176.0
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.037 266.6
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.039 50.3
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.040 125.7
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.043 100.5
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.047 88.9
Ni (mp-23) <1 1 1> <1 0 0> 0.056 106.6
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.058 201.1
SiC (mp-8062) <1 1 1> <1 0 0> 0.060 266.6
AlN (mp-661) <0 0 1> <1 0 0> 0.060 177.7
Bi2Se3 (mp-541837) <1 0 0> <1 0 0> 0.064 124.4
InSb (mp-20012) <1 0 0> <1 0 0> 0.066 88.9
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.067 231.1
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.068 284.4
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.073 92.4
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.074 213.3
AlN (mp-661) <1 1 1> <1 1 0> 0.078 201.1
LiF (mp-1138) <1 1 1> <1 0 0> 0.079 319.9
CdWO4 (mp-19387) <1 0 1> <1 1 0> 0.082 176.0
BN (mp-984) <0 0 1> <1 1 1> 0.083 215.5
CdTe (mp-406) <1 0 0> <1 0 0> 0.084 88.9
ZnO (mp-2133) <0 0 1> <1 1 1> 0.087 123.1
C (mp-48) <1 1 0> <1 1 0> 0.092 100.5
BN (mp-984) <1 0 0> <1 0 0> 0.093 231.1
Ga2O3 (mp-886) <1 1 -1> <1 0 0> 0.096 160.0
NdGaO3 (mp-3196) <0 1 0> <1 0 0> 0.096 337.7
GaTe (mp-542812) <0 0 1> <1 1 0> 0.098 75.4
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.101 284.4
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.102 276.5
TiO2 (mp-390) <1 1 1> <1 1 1> 0.103 215.5
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.104 123.1
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.105 123.1
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.107 302.2
NaCl (mp-22862) <1 0 0> <1 0 0> 0.109 160.0
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.113 226.2
Te2W (mp-22693) <1 1 0> <1 1 0> 0.114 226.2
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.114 160.0
Ga2O3 (mp-886) <0 1 0> <1 1 1> 0.114 215.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
125 113 113 0 0 0
113 125 113 0 0 0
113 113 125 0 0 0
0 0 0 26 0 0
0 0 0 0 26 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
57.8 -27.5 -27.5 0 0 0
-27.5 57.8 -27.5 0 0 0
-27.5 -27.5 57.8 0 0 0
0 0 0 37.8 0 0
0 0 0 0 37.8 0
0 0 0 0 0 37.8
Shear Modulus GV
18 GPa
Bulk Modulus KV
117 GPa
Shear Modulus GR
11 GPa
Bulk Modulus KR
117 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
117 GPa
Elastic Anisotropy
3.28
Poisson's Ratio
0.44

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1077 0.005 3
CrCoPt2 (mp-570863) 0.0466 0.034 3
LiCa6Ge (mp-12609) 0.0050 0.183 3
GaFeNi2 (mp-1065359) 0.0386 0.065 3
GaCo2Ni (mp-1018060) 0.0134 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2129 0.028 4
CrFeCoNi (mp-1012640) 0.3586 0.065 4
CrFeCoNi (mp-1096923) 0.4000 0.193 4
La3Dy (mp-972908) 0.0002 0.033 2
Sm3Ho (mp-972471) 0.0007 0.017 2
Pt3Rh (mp-974616) 0.0005 0.000 2
Ir3Ru (mp-974358) 0.0008 0.000 2
PaFe3 (mp-973908) 0.0008 0.000 2
As (mp-1096826) 0.0041 0.559 1
Sc (mp-36) 0.0015 0.048 1
Eu (mp-623532) 0.0050 0.035 1
Th (mp-37) 0.0016 0.000 1
Dy (mp-10750) 0.0048 0.021 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd Au
Final Energy/Atom
-2.8163 eV
Corrected Energy
-11.2651 eV
-11.2651 eV = -11.2651 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 611675
  • 58414
Submitted by
User remarks:
  • Gold cadmium (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)