Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.069 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.58 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.281 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 54281 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <1 0 0> 0.001 187.9
Cu (mp-30) <1 0 0> <1 0 0> 0.001 234.9
C (mp-66) <1 1 0> <1 1 0> 0.002 199.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.002 244.1
CdS (mp-672) <1 1 0> <1 1 0> 0.002 199.3
MgO (mp-1265) <1 0 0> <1 0 0> 0.002 234.9
CdS (mp-672) <0 0 1> <1 1 1> 0.005 244.1
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.011 132.9
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.013 281.8
InP (mp-20351) <1 1 0> <1 1 0> 0.013 199.3
InP (mp-20351) <1 1 1> <1 1 1> 0.013 244.1
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.014 162.7
GaN (mp-804) <0 0 1> <1 1 1> 0.021 81.4
SiC (mp-11714) <0 0 1> <1 0 0> 0.032 328.8
GaN (mp-804) <1 1 0> <1 1 0> 0.033 265.7
SiC (mp-7631) <0 0 1> <1 0 0> 0.035 328.8
Au (mp-81) <1 1 0> <1 1 0> 0.038 199.3
CsI (mp-614603) <1 1 0> <1 1 0> 0.049 265.7
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.054 332.1
CaF2 (mp-2741) <1 1 1> <1 1 0> 0.066 265.7
InAs (mp-20305) <1 0 0> <1 0 0> 0.073 187.9
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.074 81.4
Ag (mp-124) <1 1 0> <1 1 0> 0.076 199.3
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.083 187.9
GaP (mp-2490) <1 1 1> <1 1 0> 0.084 265.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.086 234.9
BN (mp-984) <1 0 0> <1 0 0> 0.087 234.9
Si (mp-149) <1 0 0> <1 0 0> 0.090 234.9
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.095 162.7
Mg (mp-153) <1 1 0> <1 1 0> 0.108 265.7
C (mp-66) <1 0 0> <1 0 0> 0.110 234.9
TiO2 (mp-390) <1 1 0> <1 1 0> 0.111 265.7
SiC (mp-8062) <1 0 0> <1 0 0> 0.112 93.9
TiO2 (mp-390) <1 0 0> <1 0 0> 0.112 187.9
Cu (mp-30) <1 1 0> <1 1 0> 0.113 199.3
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.114 332.1
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.122 332.1
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.129 187.9
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.130 332.1
PbS (mp-21276) <1 1 0> <1 1 0> 0.136 199.3
PbS (mp-21276) <1 1 1> <1 1 1> 0.136 244.1
LiF (mp-1138) <1 1 0> <1 1 0> 0.145 265.7
ZnO (mp-2133) <1 0 1> <1 1 0> 0.158 199.3
GdScO3 (mp-5690) <0 1 1> <1 1 1> 0.161 162.7
ZnO (mp-2133) <1 1 0> <1 1 0> 0.168 265.7
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.175 234.9
SiC (mp-11714) <1 0 1> <1 0 0> 0.178 328.8
NaCl (mp-22862) <1 1 1> <1 0 0> 0.181 281.8
KTaO3 (mp-3614) <1 1 1> <1 0 0> 0.181 140.9
Al (mp-134) <1 1 1> <1 0 0> 0.186 140.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
45 16 16 0 0 0
16 45 16 0 0 0
16 16 45 0 0 0
0 0 0 15 0 0
0 0 0 0 15 0
0 0 0 0 0 15
Compliance Tensor Sij (10-12Pa-1)
27.4 -7.3 -7.3 0 0 0
-7.3 27.4 -7.3 0 0 0
-7.3 -7.3 27.4 0 0 0
0 0 0 68.2 0 0
0 0 0 0 68.2 0
0 0 0 0 0 68.2
Shear Modulus GV
15 GPa
Bulk Modulus KV
26 GPa
Shear Modulus GR
15 GPa
Bulk Modulus KR
26 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
26 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.26

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.96 0.00 0.00
0.00 3.96 0.00
0.00 0.00 3.96
Dielectric Tensor εij (total)
7.52 0.00 0.00
0.00 7.52 0.00
0.00 0.00 7.52
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.96
Polycrystalline dielectric constant εpoly
(total)
7.52
Refractive Index n
1.99
Potentially ferroelectric?
Unknown

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -3.109 26.856 1.341 5.770
pack_evans_james -3.109 26.857 0.149 3.260
vinet -3.110 26.843 1.362 4.973
tait -3.109 26.839 0.150 5.392
birch_euler -3.109 26.854 0.168 0.265
pourier_tarantola -3.110 26.840 0.026 2.297
birch_lagrange -3.112 26.855 0.095 5.963
murnaghan -3.109 26.882 0.145 3.140
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiFeSb (mp-10755) 0.0000 0.000 3
LiMgAs (mp-12558) 0.0000 0.000 3
LiGaSi (mp-11390) 0.0000 0.046 3
SmSnAu (mp-13305) 0.0000 0.000 3
YbCuGe (mp-13306) 0.0000 0.162 3
TiF2 (mp-282) 0.0000 0.248 2
PuO2 (mp-1959) 0.0000 0.000 2
SnO2 (mp-12979) 0.0000 0.246 2
TbO2 (mp-2458) 0.0000 0.129 2
H2Se (mp-24420) 0.0000 0.701 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv Se
Final Energy/Atom
-3.1088 eV
Corrected Energy
-9.3265 eV
-9.3265 eV = -9.3265 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 645026
  • 168447
  • 60442
  • 645027
  • 54281
Submitted by
User remarks:
  • Sodium selenide