material

Be12Pd

ID:

mp-12666

DOI:

10.17188/1189114


Tags: Beryllium palladium (12/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.066 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.079 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.22 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Be5Pd + Be
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 109314 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.001 211.6
Al (mp-134) <1 0 0> <0 0 1> 0.002 211.6
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.003 105.8
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.006 30.4
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.008 182.5
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.008 182.5
MgF2 (mp-1249) <1 1 0> <1 1 1> 0.009 204.5
MoSe2 (mp-1634) <1 0 0> <1 1 1> 0.011 204.5
LaF3 (mp-905) <0 0 1> <1 0 0> 0.011 91.3
CsI (mp-614603) <1 1 1> <1 0 0> 0.016 212.9
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.017 304.2
LaAlO3 (mp-2920) <1 0 0> <1 1 0> 0.020 215.1
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 0 0> 0.024 182.5
CdS (mp-672) <1 0 0> <1 1 0> 0.028 86.0
CdS (mp-672) <0 0 1> <1 0 0> 0.031 30.4
Fe2O3 (mp-24972) <1 0 1> <1 1 0> 0.041 301.1
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.043 264.5
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.044 301.1
GaTe (mp-542812) <0 0 1> <1 0 0> 0.048 152.1
CdS (mp-672) <1 0 1> <1 1 0> 0.050 129.1
Mg (mp-153) <0 0 1> <1 0 0> 0.051 60.8
InP (mp-20351) <1 1 1> <1 0 0> 0.052 60.8
Cu (mp-30) <1 0 0> <0 0 1> 0.057 52.9
SiC (mp-8062) <1 0 0> <1 0 0> 0.057 365.0
Ni (mp-23) <1 0 0> <0 0 1> 0.059 211.6
SiC (mp-11714) <1 1 1> <1 1 1> 0.059 272.7
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.059 212.9
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.060 212.9
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.070 52.9
Au (mp-81) <1 1 1> <1 1 0> 0.070 301.1
SiC (mp-11714) <0 0 1> <1 0 0> 0.073 212.9
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.076 211.6
SiC (mp-7631) <0 0 1> <1 0 0> 0.079 212.9
CaF2 (mp-2741) <1 1 0> <1 0 0> 0.079 304.2
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.081 334.6
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.087 212.9
GaSe (mp-1943) <0 0 1> <1 1 1> 0.089 204.5
TiO2 (mp-390) <0 0 1> <0 0 1> 0.092 264.5
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.094 60.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.098 60.8
WS2 (mp-224) <0 0 1> <1 0 0> 0.099 60.8
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.104 212.9
GaTe (mp-542812) <1 0 0> <1 0 0> 0.106 91.3
Ag (mp-124) <1 0 0> <1 1 0> 0.109 86.0
GaP (mp-2490) <1 1 0> <1 0 0> 0.114 304.2
Ag (mp-124) <1 1 0> <1 0 0> 0.118 121.7
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.119 211.6
ZnO (mp-2133) <1 0 0> <1 1 0> 0.120 86.0
GaTe (mp-542812) <1 0 -1> <1 0 0> 0.122 152.1
LiTaO3 (mp-3666) <1 0 1> <1 1 0> 0.127 301.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
297 31 31 0 0 0
31 313 36 0 0 0
31 36 313 0 0 0
0 0 0 113 0 0
0 0 0 0 36 0
0 0 0 0 0 36
Compliance Tensor Sij (10-12Pa-1)
3.4 -0.3 -0.3 0 0 0
-0.3 3.3 -0.3 0 0 0
-0.3 -0.3 3.3 0 0 0
0 0 0 8.8 0 0
0 0 0 0 28 0
0 0 0 0 0 28
Shear Modulus GV
92 GPa
Bulk Modulus KV
124 GPa
Shear Modulus GR
63 GPa
Bulk Modulus KR
124 GPa
Shear Modulus GVRH
78 GPa
Bulk Modulus KVRH
124 GPa
Elastic Anisotropy
2.30
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nd(Al2Cu)4 (mp-974729) 0.1208 0.000 3
Pr(Al2Cu)4 (mp-862763) 0.1184 0.000 3
Sm(Al2Cu)4 (mp-16498) 0.1292 0.000 3
Ca(Al2Cu)4 (mp-10877) 0.1294 0.000 3
Th(Al2Fe)4 (mp-4703) 0.1141 0.000 3
TaBe12 (mp-567842) 0.2612 0.000 2
Be12Pt (mp-571622) 0.0234 0.119 2
Be12Nb (mp-568912) 0.2403 0.000 2
Be12Au (mp-12664) 0.2495 0.114 2
Be12Ag (mp-12665) 0.2592 0.110 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Be_sv Pd
Final Energy/Atom
-3.9163 eV
Corrected Energy
-50.9120 eV
-50.9120 eV = -50.9120 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 109314
Submitted by
User remarks:
  • Beryllium palladium (12/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)