Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.309 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.121 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnTe + Li2Te + Te |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 183.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 62.3 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 159.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 233.6 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 264.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 202.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 186.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 233.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 264.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 327.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 202.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 153.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 264.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 244.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 183.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 155.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 233.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 202.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 62.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 240.3 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 308.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 62.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 137.3 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 211.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 275.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 274.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 264.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 214.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 264.9 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 308.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 202.5 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 264.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 211.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 276.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 109.0 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 206.0 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 211.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 211.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 109.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 15.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 233.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 244.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 264.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 308.9 |
Te2W (mp-22693) | <1 1 0> | <1 1 1> | 110.5 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 53.0 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 233.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 91.8 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 211.9 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 240.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LuCuS2 (mp-1001780) | 0.3638 | 0.000 | 3 |
ScCuS2 (mp-6980) | 0.3180 | 0.000 | 3 |
HfZnN2 (mp-1014251) | 0.3248 | 0.000 | 3 |
ZrZnN2 (mp-1014244) | 0.3329 | 0.000 | 3 |
NaMnTe2 (mp-12682) | 0.4195 | 0.517 | 3 |
Li2MnV3O8 (mp-775327) | 0.5137 | 0.008 | 4 |
Li2Co3SnO8 (mp-765424) | 0.5041 | 0.203 | 4 |
Li2Mn3SnO8 (mp-772741) | 0.4975 | 0.049 | 4 |
Li2VCo3O8 (mp-761729) | 0.5034 | 0.036 | 4 |
ScAlCO (mp-1080747) | 0.2371 | 0.000 | 4 |
Mn3O4 (mp-715513) | 0.5853 | 0.000 | 2 |
Mn3O4 (mp-566607) | 0.5813 | 0.000 | 2 |
Mn3O4 (mp-18759) | 0.5758 | 0.000 | 2 |
In2Se3 (mp-19907) | 0.6348 | 0.317 | 2 |
FeO2 (mp-1097003) | 0.6224 | 1.147 | 2 |
Li4V2Cr3Fe3O16 (mp-770523) | 0.5623 | 0.264 | 5 |
Li4Ti3Mn3(NiO8)2 (mp-770507) | 0.5783 | 0.061 | 5 |
Li4Nb2V3Ni3O16 (mp-777087) | 0.5826 | 0.024 | 5 |
Li4V2Co3Cu3O16 (mp-763156) | 0.5444 | 0.088 | 5 |
Li4V2Cr3Co3O16 (mp-767986) | 0.5854 | 0.130 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Mn_pv Te |
Final Energy/Atom-4.6478 eV |
Corrected Energy-19.4353 eV
Uncorrected energy = -18.5913 eV
Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV
Corrected energy = -19.4353 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)