material

LiTlPd2

ID:

mp-12716

DOI:

10.17188/1189137


Tags: Lithium palladium thallium (1/2/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.409 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.54 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 54365 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.000 88.1
InSb (mp-20012) <1 0 0> <0 0 1> 0.000 88.1
CdTe (mp-406) <1 0 0> <0 0 1> 0.002 88.1
BN (mp-984) <0 0 1> <1 0 1> 0.008 109.1
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.008 158.5
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.009 229.0
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.010 264.2
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.011 317.1
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.013 158.5
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.014 317.1
AlN (mp-661) <1 0 1> <1 0 0> 0.015 286.5
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.016 318.3
TiO2 (mp-390) <1 0 0> <1 0 0> 0.019 222.8
GaSe (mp-1943) <1 0 0> <1 1 0> 0.020 135.1
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.026 229.0
InP (mp-20351) <1 0 0> <0 0 1> 0.027 35.2
CdS (mp-672) <0 0 1> <0 0 1> 0.031 123.3
GaN (mp-804) <1 0 1> <0 0 1> 0.035 211.4
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.037 140.9
Bi2Se3 (mp-541837) <1 0 1> <1 0 1> 0.038 254.7
Ni (mp-23) <1 0 0> <0 0 1> 0.043 158.5
Au (mp-81) <1 1 1> <0 0 1> 0.050 334.7
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.051 254.7
WSe2 (mp-1821) <1 0 1> <1 0 0> 0.051 254.7
CdS (mp-672) <1 0 1> <0 0 1> 0.053 193.8
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.073 327.4
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.078 317.1
Au (mp-81) <1 0 0> <0 0 1> 0.079 17.6
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.083 88.1
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.086 270.1
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.088 315.1
AlN (mp-661) <1 1 1> <0 0 1> 0.089 317.1
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.091 281.9
GaTe (mp-542812) <1 0 0> <1 0 1> 0.091 181.9
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.100 123.3
CdSe (mp-2691) <1 1 0> <1 0 1> 0.101 109.1
SiC (mp-8062) <1 1 0> <1 0 1> 0.108 109.1
GaSb (mp-1156) <1 1 0> <1 0 1> 0.108 109.1
LaAlO3 (mp-2920) <1 0 1> <1 1 0> 0.110 225.1
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.116 90.0
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.123 145.5
PbSe (mp-2201) <1 1 0> <1 0 1> 0.123 109.1
ZnTe (mp-2176) <1 1 0> <1 0 1> 0.126 109.1
LiNbO3 (mp-3731) <0 0 1> <1 0 1> 0.126 327.4
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.130 127.3
WSe2 (mp-1821) <1 0 0> <1 0 0> 0.134 254.7
InAs (mp-20305) <1 1 0> <1 0 1> 0.135 109.1
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.137 70.5
MoSe2 (mp-1634) <1 0 0> <1 0 0> 0.142 254.7
ZnO (mp-2133) <1 1 1> <0 0 1> 0.143 281.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
125 77 83 0 0 0
77 125 83 0 0 0
83 83 129 0 0 0
0 0 0 47 0 0
0 0 0 0 47 0
0 0 0 0 0 51
Compliance Tensor Sij (10-12Pa-1)
15.8 -5.1 -6.9 0 0 0
-5.1 15.8 -6.9 0 0 0
-6.9 -6.9 16.7 0 0 0
0 0 0 21.4 0 0
0 0 0 0 21.4 0
0 0 0 0 0 19.5
Shear Modulus GV
38 GPa
Bulk Modulus KV
96 GPa
Shear Modulus GR
33 GPa
Bulk Modulus KR
96 GPa
Shear Modulus GVRH
35 GPa
Bulk Modulus KVRH
96 GPa
Elastic Anisotropy
0.77
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
GaCuPt2 (mp-644280) 0.1504 0.000 3
VSnRh2 (mp-669918) 0.0268 0.011 3
FeCuPt2 (mp-3702) 0.0156 0.017 3
CrSnRh2 (mp-1018066) 0.1471 0.176 3
AlCuPt2 (mp-12550) 0.2232 0.000 3
Cr8Ni50Mo15W2 (mp-767372) 0.5545 0.028 4
CrFeCoNi (mp-1012640) 0.5217 0.118 4
CrFeCoNi (mp-1096923) 0.5566 0.193 4
BiH3 (mp-984050) 0.0064 0.656 2
Rb3Nb (mp-974869) 0.0121 1.188 2
ZnBi3 (mp-971718) 0.0064 0.175 2
CuAu (mp-522) 0.0063 0.000 2
LiBi (mp-22902) 0.0156 0.000 2
Hg (mp-975272) 0.4632 0.001 1
K (mp-972981) 0.3833 0.008 1
Hg (mp-569360) 0.3869 0.001 1
Eu (mp-1057315) 0.4141 0.000 1
Pr (mp-1009594) 0.4619 0.032 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Tl_d Pd
Final Energy/Atom
-4.0644 eV
Corrected Energy
-16.2576 eV
Uncorrected energy = -16.2576 eV Corrected energy = -16.2576 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 54365
Submitted by
User remarks:
  • Lithium palladium thallium (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)