Final Magnetic Moment2.923 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.141 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/m [10] |
Hall-P 2y |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 158.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 158.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 143.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 168.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 84.2 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 239.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 68.0 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 191.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 90.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 42.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 168.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 226.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 228.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 191.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 277.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 126.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 113.4 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 192.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 337.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 47.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 268.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 340.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 84.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 239.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 95.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 45.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 230.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 268.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 268.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 168.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 191.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 339.5 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 337.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 113.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 22.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 226.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 228.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 334.9 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 345.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 208.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 339.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 272.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 226.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 68.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 92.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 294.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 246.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 287.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 268.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 268.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2GeTeO6 (mp-10340) | 0.7030 | 0.000 | 4 |
Li2VO2F (mp-763209) | 0.7407 | 0.096 | 4 |
Li2VO2F (mp-763203) | 0.7056 | 0.102 | 4 |
Li2VO2F (mp-763345) | 0.7380 | 0.101 | 4 |
Li6NbFe5O12 (mp-765619) | 0.7353 | 0.059 | 4 |
Te3Pt2 (mp-570562) | 0.7461 | 0.008 | 2 |
Te2Au (mp-20123) | 0.6122 | 0.000 | 2 |
Nb2C (mp-569989) | 0.7420 | 0.000 | 2 |
TlPt2Se3 (mp-541487) | 0.6425 | 0.000 | 3 |
Na2TeSe3 (mp-573581) | 0.6821 | 0.000 | 3 |
TlTe3Pt2 (mp-9251) | 0.5228 | 0.000 | 3 |
TlPd2Se3 (mp-7038) | 0.6805 | 0.000 | 3 |
Mn2O3F (mp-767610) | 0.6354 | 0.065 | 3 |
Li4Mn2TeWO12 (mp-768044) | 0.7493 | 0.059 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points72 |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv Te Au |
Final Energy/Atom-4.3881 eV |
Corrected Energy-26.3284 eV
-26.3284 eV = -26.3284 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)