material

CdTe

ID:

mp-12779

DOI:

10.17188/1189186


Tags: Cadmium telluride - thin film Cadmium telluride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.663 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.006 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.47 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CdTe
Band Gap
0.619 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 150941 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.000 76.0
SiC (mp-8062) <1 1 1> <0 0 1> 0.000 133.0
CdTe (mp-406) <1 1 1> <0 0 1> 0.001 76.0
Au (mp-81) <1 1 1> <0 0 1> 0.001 361.1
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.002 57.0
GaAs (mp-2534) <1 1 0> <1 1 0> 0.003 186.8
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.003 186.8
InSb (mp-20012) <1 1 1> <0 0 1> 0.003 76.0
Ag (mp-124) <1 1 1> <0 0 1> 0.006 361.1
AlN (mp-661) <0 0 1> <0 0 1> 0.006 76.0
GaAs (mp-2534) <1 1 1> <0 0 1> 0.010 57.0
GaN (mp-804) <0 0 1> <0 0 1> 0.010 171.0
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.011 361.1
InP (mp-20351) <1 1 1> <0 0 1> 0.011 247.0
SiC (mp-11714) <1 0 0> <1 0 0> 0.012 251.6
Ge (mp-32) <1 1 0> <1 1 0> 0.017 186.8
LiF (mp-1138) <1 0 0> <0 0 1> 0.020 133.0
YVO4 (mp-19133) <1 1 1> <1 1 0> 0.023 249.0
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.025 65.1
GaAs (mp-2534) <1 0 0> <0 0 1> 0.026 361.1
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.027 152.0
Al (mp-134) <1 0 0> <1 1 1> 0.028 65.1
Mg (mp-153) <1 0 1> <1 0 1> 0.030 284.6
YVO4 (mp-19133) <0 0 1> <1 1 1> 0.030 260.4
ZnO (mp-2133) <1 0 1> <1 0 0> 0.033 179.7
Ge (mp-32) <1 1 1> <0 0 1> 0.037 57.0
BN (mp-984) <0 0 1> <0 0 1> 0.038 171.0
KCl (mp-23193) <1 0 0> <1 1 1> 0.039 325.5
C (mp-48) <0 0 1> <0 0 1> 0.039 133.0
SiC (mp-7631) <1 0 1> <1 0 0> 0.042 143.8
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.043 203.3
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.043 203.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.046 76.0
SiO2 (mp-6930) <1 1 0> <1 0 1> 0.048 284.6
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.051 325.3
PbS (mp-21276) <1 1 1> <0 0 1> 0.053 247.0
TeO2 (mp-2125) <1 1 0> <1 1 1> 0.056 195.3
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.056 186.8
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.057 249.0
Si (mp-149) <1 0 0> <1 0 0> 0.059 179.7
TePb (mp-19717) <1 0 0> <1 0 0> 0.059 215.7
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.059 179.7
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.059 179.7
ZnO (mp-2133) <1 1 1> <1 0 0> 0.059 287.6
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.059 71.9
Si (mp-149) <1 1 1> <1 1 0> 0.060 311.3
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.060 249.0
CeO2 (mp-20194) <1 1 1> <1 1 0> 0.060 311.3
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.061 186.8
TePb (mp-19717) <1 1 0> <0 0 1> 0.065 304.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
54 27 23 0 0 0
27 54 23 0 0 0
23 23 62 0 0 0
0 0 0 11 0 0
0 0 0 0 11 0
0 0 0 0 0 13
Compliance Tensor Sij (10-12Pa-1)
26.9 -11.3 -5.7 0 0 0
-11.3 26.9 -5.7 0 0 0
-5.7 -5.7 20.3 0 0 0
0 0 0 91.7 0 0
0 0 0 0 91.7 0
0 0 0 0 0 76.4
Shear Modulus GV
13 GPa
Bulk Modulus KV
35 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
35 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
35 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.33

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -0.01350 0.00000
0.00000 0.00000 0.00000 -0.01350 0.00000 0.00000
-0.04397 -0.04397 0.01061 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.06308 C/m2
Crystallographic Direction vmax
0.00000
-0.00000
-1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
8.92 0.00 0.00
0.00 8.92 0.00
0.00 0.00 8.90
Dielectric Tensor εij (total)
12.08 0.00 0.00
0.00 12.08 0.00
0.00 0.00 12.58
Polycrystalline dielectric constant εpoly
(electronic contribution)
8.91
Polycrystalline dielectric constant εpoly
(total)
12.25
Refractive Index n
2.98
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BeSiN2 (mp-7913) 0.0624 0.000 3
LiInSe2 (mp-20310) 0.1012 0.001 3
MgSnN2 (mp-1029791) 0.1555 0.000 3
ZnSnN2 (mp-1029469) 0.0653 0.000 3
Zn2SbN3 (mp-1029334) 0.1460 0.020 3
CoCu2SiS4 (mp-556830) 0.3096 0.065 4
Li2ZnSnS4 (mp-555186) 0.1903 0.000 4
ZnGaNO (mp-558481) 0.2880 0.058 4
ZnCu2GeS4 (mp-6408) 0.3032 0.000 4
CoCu2SiS4 (mp-11769) 0.3056 0.065 4
AlP (mp-8880) 0.0072 0.005 2
MgGa (mp-1094992) 0.0038 0.664 2
HgS (mp-973676) 0.0097 0.002 2
ZnS (mp-560588) 0.0038 0.003 2
InP (mp-966800) 0.0025 0.004 2
Ge (mp-1007760) 0.0259 0.022 1
Si (mp-165) 0.0361 0.013 1
C (mp-611426) 0.2249 0.146 1
C (mp-47) 0.0448 0.162 1
Ge (mp-1091415) 0.2379 0.014 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Preparation of CdS from CdCl2 and MA: Aqueous solution containing equal amount of CdCl2 and MA was added NaOH to adjust the pH to 5.74, which was equal to the CdTe NCs solution. After that, the soluti [...]
CdTe nanoparticle-sensitized TiO2 nanotube arrays (CdTe/TiO2 NTAs) were prepared by combining the solgel method with the electrodeposition method by the aid of anodic aluminum oxide template. The mor [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition CdTe.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd Te
Final Energy/Atom
-2.4854 eV
Corrected Energy
-10.7858 eV
Uncorrected energy = -9.9418 eV Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV Corrected energy = -10.7858 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 150941
  • 620518
  • 620534
Submitted by
User remarks:
  • Cadmium telluride - thin film

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)