material

Ni3Pt

ID:

mp-12798

DOI:

10.17188/1189201


Tags: Nickel platinum (3/1)

Material Details

Final Magnetic Moment
2.369 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.069 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
< 0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.69 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ni3Pt
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 151193 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 1 0> <1 1 0> 0.000 150.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.002 207.1
Si (mp-149) <1 0 0> <1 0 0> 0.002 119.8
Si (mp-149) <1 1 0> <1 1 0> 0.002 169.4
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.003 119.8
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.003 169.4
Ge (mp-32) <1 0 0> <1 0 0> 0.004 66.6
LiF (mp-1138) <1 0 0> <1 0 0> 0.004 66.6
Al (mp-134) <1 1 0> <1 1 0> 0.006 207.1
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.008 66.6
TePb (mp-19717) <1 0 0> <1 0 0> 0.010 173.1
TePb (mp-19717) <1 1 1> <1 1 1> 0.011 299.7
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.015 106.5
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.016 150.6
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.022 207.1
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.027 207.1
C (mp-48) <1 0 0> <1 0 0> 0.034 173.1
GaAs (mp-2534) <1 0 0> <1 0 0> 0.036 66.6
LiGaO2 (mp-5854) <1 1 1> <1 1 1> 0.048 276.7
Fe2O3 (mp-24972) <1 0 0> <1 0 0> 0.048 213.0
CdS (mp-672) <1 1 0> <1 1 0> 0.050 150.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.068 69.2
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.069 23.1
WS2 (mp-224) <1 0 0> <1 1 0> 0.070 225.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.072 66.6
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.074 169.4
C (mp-48) <0 0 1> <1 1 1> 0.079 69.2
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.079 173.1
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.081 150.6
Fe2O3 (mp-24972) <1 0 1> <1 0 0> 0.088 226.3
Mg (mp-153) <1 1 1> <1 0 0> 0.092 119.8
LaF3 (mp-905) <1 0 1> <1 0 0> 0.094 213.0
GaTe (mp-542812) <1 0 0> <1 1 0> 0.095 225.9
TiO2 (mp-390) <1 0 0> <1 0 0> 0.097 332.8
Te2W (mp-22693) <1 1 0> <1 1 0> 0.110 113.0
LaF3 (mp-905) <1 0 0> <1 0 0> 0.119 53.2
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.121 56.5
Al2O3 (mp-1143) <0 0 1> <1 1 0> 0.123 301.2
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.123 69.2
GaP (mp-2490) <1 0 0> <1 0 0> 0.130 119.8
LiTaO3 (mp-3666) <1 0 1> <1 0 0> 0.138 226.3
GaP (mp-2490) <1 1 0> <1 1 0> 0.139 169.4
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.142 133.1
NdGaO3 (mp-3196) <1 0 1> <1 1 0> 0.143 320.0
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.154 133.1
TiO2 (mp-390) <1 0 1> <1 1 1> 0.160 276.7
Ge (mp-32) <1 1 0> <1 0 0> 0.162 332.8
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.170 131.8
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.181 131.8
NdGaO3 (mp-3196) <0 1 1> <1 1 0> 0.188 263.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
285 167 167 0 0 0
167 285 167 0 0 0
167 167 285 0 0 0
0 0 0 124 0 0
0 0 0 0 124 0
0 0 0 0 0 124
Compliance Tensor Sij (10-12Pa-1)
6.2 -2.3 -2.3 0 0 0
-2.3 6.2 -2.3 0 0 0
-2.3 -2.3 6.2 0 0 0
0 0 0 8.1 0 0
0 0 0 0 8.1 0
0 0 0 0 0 8.1
Shear Modulus GV
98 GPa
Bulk Modulus KV
206 GPa
Shear Modulus GR
86 GPa
Bulk Modulus KR
206 GPa
Shear Modulus GVRH
92 GPa
Bulk Modulus KVRH
206 GPa
Elastic Anisotropy
0.69
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.000 3
LiCa6Ge (mp-12609) 0.0000 0.180 3
GaFeNi2 (mp-1065359) 0.0412 0.066 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.118 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
CaTl3 (mp-526) 0.0000 0.000 2
ZrH3 (mp-972087) 0.0000 0.122 2
GdPd3 (mp-1064256) 0.0000 0.000 2
USi3 (mp-2800) 0.0000 0.000 2
Mg3Zr (mp-1094792) 0.0000 0.052 2
H2 (mp-634659) 0.0000 0.000 1
Sn (mp-1022725) 0.0000 0.037 1
N2 (mp-1056857) 0.0000 0.000 1
Cd (mp-1096861) 0.0000 0.001 1
Pd (mp-1056438) 0.0000 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ni_pv Pt
Final Energy/Atom
-5.9214 eV
Corrected Energy
-23.6854 eV
-23.6854 eV = -23.6854 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 151193
Submitted by
User remarks:
  • Nickel platinum (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)