Final Magnetic Moment1.954 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.621 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.521 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYbS2 + YbS |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 350.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 233.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 194.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 272.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 116.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 155.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 272.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 194.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 272.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 272.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 194.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 272.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 194.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 155.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 194.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 350.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 311.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 311.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 272.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 272.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 194.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 194.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 116.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 272.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 194.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 116.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 116.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 38.9 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 116.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 311.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 194.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 116.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 350.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 272.3 |
BN (mp-984) | <1 1 1> | <0 0 1> | 311.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 116.7 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 311.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 155.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 272.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 194.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 155.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 272.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 272.3 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 155.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 272.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 194.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 350.1 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 155.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 311.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 272.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgGeO3 (mp-3759) | 0.5288 | 0.064 | 3 |
CaSnS3 (mp-866826) | 0.4968 | 0.072 | 3 |
LiMgH3 (mp-23736) | 0.5191 | 0.009 | 3 |
MnSnO3 (mp-25005) | 0.5249 | 0.000 | 3 |
NaCaH3 (mp-1078933) | 0.4787 | 0.070 | 3 |
Mg2TaWO6 (mvc-5863) | 0.6268 | 0.100 | 4 |
Mg2VWO6 (mvc-5881) | 0.6083 | 0.018 | 4 |
Mg2MoWO6 (mvc-5910) | 0.6204 | 0.031 | 4 |
Mg2CrWO6 (mvc-5960) | 0.6073 | 0.047 | 4 |
InNi2SbO6 (mp-1078367) | 0.5552 | 0.000 | 4 |
In2S3 (mp-22375) | 0.5443 | 0.023 | 2 |
Sc2O3 (mp-755313) | 0.5540 | 0.039 | 2 |
Yb3N2 (mp-864675) | 0.5480 | 0.000 | 2 |
Y2O3 (mp-754759) | 0.5439 | 0.051 | 2 |
In2O3 (mp-22323) | 0.5532 | 0.029 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.7282 | 0.083 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 S |
Final Energy/Atom-4.3206 eV |
Corrected Energy-47.1869 eV
-47.1869 eV = -43.2062 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)