Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.024 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.107 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlPO4 |
Band Gap5.272 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 183.3 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 274.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 282.7 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 282.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 233.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 233.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 274.8 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 50.4 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 206.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 281.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 219.8 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 168.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 31.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 140.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 197.1 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 201.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 282.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 118.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 122.2 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 305.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 197.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 197.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 183.3 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 168.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 157.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 197.1 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 168.8 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 183.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 157.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 118.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 197.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 219.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 281.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 157.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 201.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 280.2 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 168.8 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 281.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 305.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 183.3 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 112.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 157.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 140.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 183.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 251.3 |
BN (mp-984) | <1 1 1> | <1 0 1> | 244.4 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 252.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 94.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 219.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 201.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoSeO4 (mp-555138) | 0.1448 | 0.005 | 3 |
CuSeO4 (mp-554109) | 0.1368 | 0.002 | 3 |
MgSeO4 (mp-12630) | 0.1647 | 0.002 | 3 |
TiSiO4 (mp-1095481) | 0.1343 | 0.156 | 3 |
FePO4 (mp-25527) | 0.1917 | 0.027 | 3 |
LiFe2(PO4)3 (mp-699352) | 0.2882 | 0.376 | 4 |
LiNi2(PO4)3 (mp-32397) | 0.2772 | 0.238 | 4 |
LiCr2(PO4)3 (mp-31677) | 0.3565 | 0.068 | 4 |
LiCr2(PO4)3 (mp-697765) | 0.2661 | 0.068 | 4 |
LiMn2(PO4)3 (mp-697768) | 0.3315 | 0.163 | 4 |
FeO2 (mvc-11999) | 0.5072 | 0.720 | 2 |
CrO2 (mvc-11581) | 0.3528 | 0.166 | 2 |
VO2 (mp-777469) | 0.2891 | 0.038 | 2 |
VO2 (mvc-6918) | 0.3277 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.3967 | 0.281 | 2 |
Li6MnV3(PO4)6 (mp-775325) | 0.5622 | 0.030 | 5 |
Li3MnV(PO4)3 (mp-772102) | 0.5637 | 0.145 | 5 |
LiCrPO4F (mp-770575) | 0.5436 | 0.054 | 5 |
Li3MnV(PO4)3 (mp-778888) | 0.5768 | 0.044 | 5 |
Cr2CoNi3(PO4)6 (mp-763120) | 0.5675 | 0.115 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6189 | 0.257 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.6706 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.7205 | 0.020 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.7050 | 0.008 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.6450 | 0.000 | 6 |
Explore more synthesis descriptions for materials of composition AlPO4.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al P O |
Final Energy/Atom-7.3814 eV |
Corrected Energy-94.1951 eV
-94.1951 eV = -88.5768 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)