material

Cu2SnTe3

ID:

mp-13089

DOI:

10.17188/1189375


Tags: Dicopper tin telluride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.140 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.016 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.91 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cu5Sn2Te7 + SnTe
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Imm2 [44]
Hall
I 2 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 160882 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Bi2Se3 (mp-541837) <0 0 1> <1 1 0> 0.003 197.4
Al (mp-134) <1 1 1> <1 1 0> 0.004 197.4
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.004 197.4
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 0> 0.005 197.4
BN (mp-984) <0 0 1> <1 1 0> 0.007 98.7
ZnO (mp-2133) <0 0 1> <1 1 0> 0.007 197.4
SiO2 (mp-6930) <0 0 1> <1 1 0> 0.015 197.4
InAs (mp-20305) <1 1 1> <1 1 0> 0.018 197.4
AlN (mp-661) <1 1 1> <0 1 1> 0.024 254.9
ZnTe (mp-2176) <1 1 1> <1 1 0> 0.025 197.4
TiO2 (mp-2657) <0 0 1> <0 1 0> 0.027 173.2
Ag (mp-124) <1 0 0> <0 1 0> 0.027 173.2
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.027 188.7
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.028 240.1
SiC (mp-8062) <1 0 0> <0 1 0> 0.031 57.7
CdSe (mp-2691) <1 0 0> <0 1 0> 0.031 115.5
Ni (mp-23) <1 1 1> <1 1 0> 0.032 296.1
CaCO3 (mp-3953) <0 0 1> <1 1 0> 0.033 197.4
TePb (mp-19717) <1 0 0> <0 1 0> 0.034 173.2
LaF3 (mp-905) <1 0 0> <0 1 1> 0.036 318.6
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.037 253.4
Au (mp-81) <1 0 0> <0 1 0> 0.038 173.2
GaSb (mp-1156) <1 0 0> <0 1 0> 0.039 115.5
MgF2 (mp-1249) <1 0 1> <0 1 1> 0.040 318.6
C (mp-66) <1 1 1> <1 1 0> 0.042 197.4
ZnTe (mp-2176) <1 0 0> <0 1 0> 0.043 115.5
CdS (mp-672) <0 0 1> <1 1 0> 0.044 197.4
Te2Mo (mp-602) <1 1 1> <0 0 1> 0.044 188.7
InAs (mp-20305) <1 0 0> <0 1 0> 0.049 115.5
InAs (mp-20305) <1 1 0> <0 0 1> 0.053 53.9
PbSe (mp-2201) <1 0 0> <0 1 0> 0.054 115.5
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.055 53.9
ZrO2 (mp-2858) <1 0 -1> <0 1 0> 0.057 288.7
C (mp-66) <1 1 0> <0 0 1> 0.062 53.9
SiC (mp-8062) <1 1 0> <0 0 1> 0.065 27.0
Ga2O3 (mp-886) <0 1 0> <0 0 1> 0.066 215.7
YAlO3 (mp-3792) <1 1 1> <1 0 1> 0.067 253.4
CdS (mp-672) <1 1 0> <0 0 1> 0.072 296.6
SiC (mp-7631) <1 0 1> <0 0 1> 0.080 188.7
C (mp-48) <0 0 1> <0 0 1> 0.083 215.7
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.086 350.5
Mg (mp-153) <1 0 1> <0 0 1> 0.086 188.7
NdGaO3 (mp-3196) <1 0 1> <0 1 1> 0.090 318.6
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.098 350.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.105 197.4
LiTaO3 (mp-3666) <1 1 0> <1 0 1> 0.105 253.4
MgO (mp-1265) <1 1 1> <0 0 1> 0.108 188.7
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.110 240.1
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.110 134.8
CdSe (mp-2691) <1 1 0> <0 0 1> 0.116 53.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
61 36 39 0 0 0
36 80 23 0 0 0
39 23 75 0 0 0
0 0 0 13 0 0
0 0 0 0 26 0
0 0 0 0 0 27
Compliance Tensor Sij (10-12Pa-1)
30.2 -9.9 -12.6 0 0 0
-9.9 16.9 -0.1 0 0 0
-12.6 -0.1 19.8 0 0 0
0 0 0 76 0 0
0 0 0 0 37.8 0
0 0 0 0 0 36.5
Shear Modulus GV
21 GPa
Bulk Modulus KV
46 GPa
Shear Modulus GR
19 GPa
Bulk Modulus KR
46 GPa
Shear Modulus GVRH
20 GPa
Bulk Modulus KVRH
46 GPa
Elastic Anisotropy
0.75
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
In11Cu9Se20 (mp-677803) 0.1994 0.031 3
Cu2SnTe3 (mp-675880) 0.1401 0.018 3
Cu2SnSe3 (mp-11658) 0.1301 0.014 3
Cu2SnS3 (mp-10519) 0.1539 0.000 3
MgSiAs2 (mp-1016197) 0.2075 0.000 3
Cu2SnHgS4 (mp-1025467) 0.2104 0.000 4
Cu2HgGeSe4 (mp-12855) 0.2342 0.000 4
CdCu2SnS4 (mp-1078292) 0.2290 0.000 4
CdCu2GeTe4 (mp-1078909) 0.2267 0.006 4
Cu2SnHgSe4 (mp-16566) 0.2128 0.000 4
ZnP2 (mp-2782) 0.2463 0.000 2
ZnP2 (mp-11025) 0.2448 0.000 2
BC5 (mp-1077743) 0.2291 0.265 2
BC7 (mp-1079046) 0.2244 0.240 2
BC7 (mp-1079661) 0.2804 0.239 2
Sn (mp-949028) 0.2889 0.012 1
Si (mp-971662) 0.2887 0.062 1
Si (mp-1079297) 0.3679 0.072 1
C (mp-1078845) 0.3336 0.266 1
C (mp-1080826) 0.3365 0.299 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv Sn_d Te
Final Energy/Atom
-3.7438 eV
Corrected Energy
-23.7289 eV
Uncorrected energy = -22.4629 eV Composition-based energy adjustment (-0.422 eV/atom x 3.0 atoms) = -1.2660 eV Corrected energy = -23.7289 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 160882
Submitted by
User remarks:
  • Dicopper tin telluride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)