Final Magnetic Moment-0.774 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-0.983 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr + Cr3S4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP31c [163] |
Hall-P 3 2c |
Point Group3m |
Crystal Systemtrigonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 214.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 204.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 214.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 214.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 136.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 275.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 214.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 275.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 367.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 68.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 214.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 275.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 244.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 367.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 214.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 275.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 298.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 275.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 122.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 224.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 336.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 118.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 153.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 224.1 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 224.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 153.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 214.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 298.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 244.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 244.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 367.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 68.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 122.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 153.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 214.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 214.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 214.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 91.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 367.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr2SiO6 (mp-762403) | 0.4785 | 0.060 | 4 |
Li2Al2FeO6 (mp-770845) | 0.5252 | 0.093 | 4 |
Li3VFe3O8 (mp-763971) | 0.5444 | 0.068 | 4 |
Li3CrFe3O8 (mp-763933) | 0.5278 | 0.071 | 4 |
Li4Co5SnO12 (mp-771202) | 0.5149 | 0.038 | 4 |
Ti9O8 (mp-32544) | 0.5744 | 0.126 | 2 |
Cr7Se8 (mp-696673) | 0.2645 | 0.061 | 2 |
V3Te4 (mp-1028) | 0.4669 | 0.000 | 2 |
Ti9S10 (mp-673637) | 0.5614 | 0.040 | 2 |
Fe3Se4 (mp-2780) | 0.4735 | 0.078 | 2 |
V2NiS4 (mp-4909) | 0.4868 | 0.002 | 3 |
Ca3(TiS2)4 (mvc-16041) | 0.4744 | 0.142 | 3 |
V2CrTe4 (mp-1025278) | 0.4548 | 0.009 | 3 |
Ti2CrTe4 (mp-1025345) | 0.4870 | 0.049 | 3 |
Li2(CoO2)3 (mp-705847) | 0.4704 | 0.057 | 3 |
Li6Mn3Cr2Fe3O16 (mp-868267) | 0.6278 | 0.076 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points8 |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv S |
Final Energy/Atom-7.2539 eV |
Corrected Energy-167.5470 eV
-167.5470 eV = -159.5855 eV (uncorrected energy) - 7.9615 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)