material

YMgCu4

ID:

mp-13172

DOI:

10.17188/1189434


Tags: Yttrium magnesium copper (1/1/4) Yttrium copper magnesium (1/4/1) - tau1

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.234 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.47 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 1 0> <1 1 0> 0.000 73.8
Au (mp-81) <1 1 1> <1 1 1> 0.000 90.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.000 260.9
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.000 208.7
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.001 52.2
Ni (mp-23) <1 0 0> <1 0 0> 0.003 208.7
Ni (mp-23) <1 1 0> <1 1 0> 0.003 295.2
Cu (mp-30) <1 0 0> <1 0 0> 0.003 52.2
Cu (mp-30) <1 1 0> <1 1 0> 0.003 73.8
Cu (mp-30) <1 1 1> <1 1 1> 0.003 90.4
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.003 208.7
Mg (mp-153) <0 0 1> <1 1 1> 0.007 271.2
Ag (mp-124) <1 1 0> <1 1 0> 0.013 73.8
Ag (mp-124) <1 1 1> <1 1 1> 0.013 90.4
GaTe (mp-542812) <1 0 1> <1 1 0> 0.020 295.2
NaCl (mp-22862) <1 0 0> <1 0 0> 0.023 260.9
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.033 271.2
WS2 (mp-224) <0 0 1> <1 1 1> 0.034 271.2
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.039 221.4
BaF2 (mp-1029) <1 1 1> <1 1 1> 0.040 271.2
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.042 260.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.043 221.4
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.044 260.9
PbSe (mp-2201) <1 1 0> <1 1 0> 0.046 221.4
PbSe (mp-2201) <1 1 1> <1 1 1> 0.047 271.2
Te2W (mp-22693) <1 1 0> <1 1 0> 0.051 221.4
ZrO2 (mp-2858) <0 1 0> <1 1 0> 0.059 221.4
SiC (mp-11714) <1 0 0> <1 1 0> 0.060 221.4
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.061 260.9
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.071 208.7
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.071 90.4
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.073 271.2
GaSb (mp-1156) <1 1 0> <1 1 0> 0.074 221.4
GaSb (mp-1156) <1 1 1> <1 1 1> 0.074 271.2
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.086 260.9
CdS (mp-672) <1 1 0> <1 1 0> 0.094 147.6
GaAs (mp-2534) <1 0 0> <1 0 0> 0.096 260.9
AlN (mp-661) <0 0 1> <1 1 0> 0.096 295.2
CdSe (mp-2691) <1 1 0> <1 1 0> 0.100 221.4
CdSe (mp-2691) <1 1 1> <1 1 1> 0.102 271.2
Te2Mo (mp-602) <0 0 1> <1 1 0> 0.110 221.4
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.125 260.9
Al (mp-134) <1 0 0> <1 0 0> 0.128 208.7
Te2Mo (mp-602) <1 0 0> <1 1 0> 0.130 221.4
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.131 104.4
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.136 260.9
Ge(Bi3O5)4 (mp-23352) <1 1 0> <1 1 0> 0.137 147.6
Te2W (mp-22693) <0 0 1> <1 1 0> 0.149 221.4
BN (mp-984) <1 1 0> <1 1 1> 0.163 271.2
Ge (mp-32) <1 0 0> <1 0 0> 0.168 260.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
136 70 70 0 0 0
70 136 70 0 0 0
70 70 136 0 0 0
0 0 0 50 0 0
0 0 0 0 50 0
0 0 0 0 0 50
Compliance Tensor Sij (10-12Pa-1)
11.3 -3.8 -3.8 0 0 0
-3.8 11.3 -3.8 0 0 0
-3.8 -3.8 11.3 0 0 0
0 0 0 19.8 0 0
0 0 0 0 19.8 0
0 0 0 0 0 19.8
Shear Modulus GV
43 GPa
Bulk Modulus KV
92 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
92 GPa
Shear Modulus GVRH
43 GPa
Bulk Modulus KVRH
92 GPa
Elastic Anisotropy
0.21
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeMnNi4 (mp-990536) 0.0021 0.034 3
UZnNi4 (mp-21899) 0.0021 0.000 3
SmCu4Ag (mp-867863) 0.0005 0.000 3
GdMgNi4 (mp-977381) 0.0021 0.000 3
CeMgNi4 (mp-13435) 0.0021 0.000 3
DyCu5 (mp-30578) 0.0021 0.004 2
HoCu5 (mp-580364) 0.0029 0.007 2
ErCu5 (mp-30579) 0.0052 0.000 2
TbCu5 (mp-1077262) 0.0023 0.007 2
ZrNi5 (mp-905383) 0.0030 0.001 2
Co (mp-1072089) 0.0349 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Mg_pv Cu_pv
Final Energy/Atom
-4.3114 eV
Corrected Energy
-25.8683 eV
-25.8683 eV = -25.8683 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 163696
  • 191559
Submitted by
User remarks:
  • Yttrium copper magnesium (1/4/1) - tau1

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)