Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.624 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.273 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZrTe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 211.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 213.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 193.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 229.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 302.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 253.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 157.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 243.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 98.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 229.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 229.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 91.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 108.8 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 196.7 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 196.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 157.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 253.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 91.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 229.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 91.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 229.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 120.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 169.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 193.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 36.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 133.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 196.7 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 270.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 84.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 120.9 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 229.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 253.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 335.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 91.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 169.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 263.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 193.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 213.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 91.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 84.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 48.3 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 316.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 326.4 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 262.2 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 262.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 213.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 326.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 84.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 158.3 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 105.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
90 | 40 | 65 | 0 | 0 | 0 |
40 | 90 | 65 | 0 | 0 | 0 |
65 | 65 | 118 | 0 | 0 | 0 |
0 | 0 | 0 | 59 | 0 | 0 |
0 | 0 | 0 | 0 | 59 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
18.6 | -1.4 | -9.6 | 0 | 0 | 0 |
-1.4 | 18.6 | -9.6 | 0 | 0 | 0 |
-9.6 | -9.6 | 19.1 | 0 | 0 | 0 |
0 | 0 | 0 | 16.9 | 0 | 0 |
0 | 0 | 0 | 0 | 16.9 | 0 |
0 | 0 | 0 | 0 | 0 | 40 |
Shear Modulus GV37 GPa |
Bulk Modulus KV71 GPa |
Shear Modulus GR28 GPa |
Bulk Modulus KR65 GPa |
Shear Modulus GVRH33 GPa |
Bulk Modulus KVRH68 GPa |
Elastic Anisotropy1.63 |
Poisson's Ratio0.29 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaNbO2 (mp-3744) | 0.7147 | 0.000 | 3 |
NaNbSe2 (mp-7939) | 0.6507 | 0.000 | 3 |
NaNbS2 (mp-7937) | 0.6963 | 0.000 | 3 |
Ca3SiBr2 (mp-567974) | 0.6672 | 0.276 | 3 |
TiTe (mp-599) | 0.1855 | 0.335 | 2 |
TcB (mp-999120) | 0.3140 | 0.163 | 2 |
ReN (mp-999266) | 0.1779 | 0.374 | 2 |
NiBi (mp-22861) | 0.2845 | 0.303 | 2 |
ZrTe (mp-569544) | 0.1781 | 0.055 | 2 |
Xe (mp-979286) | 0.6942 | 0.006 | 1 |
N2 (mp-1061298) | 0.7135 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Te |
Final Energy/Atom-6.4698 eV |
Corrected Energy-25.8793 eV
-25.8793 eV = -25.8793 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)