Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.794 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrSbO4 |
Band Gap2.203 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 278.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 218.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 348.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 218.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 130.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 134.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 174.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 218.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 87.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 55.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 278.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 130.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 43.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 305.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 269.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 348.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 67.0 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 178.9 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 244.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 305.3 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 295.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 43.6 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 305.3 |
GaSe (mp-1943) | <1 0 0> | <1 1 1> | 269.1 |
GaSe (mp-1943) | <1 0 1> | <1 0 -1> | 278.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 174.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 305.3 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 223.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 178.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 334.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 269.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 278.7 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 111.5 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 55.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 55.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 43.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 55.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 130.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 134.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 55.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 295.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 167.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 111.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 278.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 334.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 130.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 55.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 348.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PrTaO4 (mp-17722) | 0.1654 | 0.000 | 3 |
NdTaO4 (mp-18433) | 0.1629 | 0.015 | 3 |
EuSbO4 (mp-510637) | 0.1556 | 0.000 | 3 |
NdSbO4 (mp-13195) | 0.0654 | 0.000 | 3 |
SmSbO4 (mp-13196) | 0.1605 | 0.000 | 3 |
Na2MnCrF7 (mp-617603) | 0.5898 | 0.000 | 4 |
NaW6CCl18 (mp-567182) | 0.5996 | 0.000 | 4 |
LiW6CCl18 (mp-571612) | 0.5963 | 0.012 | 4 |
LaFeReO6 (mvc-8995) | 0.5999 | 0.296 | 4 |
YCo(WO4)2 (mvc-587) | 0.5859 | 0.173 | 4 |
Bi3O5 (mp-753707) | 0.7128 | 0.059 | 2 |
BiO2 (mp-557993) | 0.5918 | 0.000 | 2 |
SbO2 (mp-560098) | 0.6772 | 0.001 | 2 |
Bi3O7 (mvc-9064) | 0.7039 | 0.141 | 2 |
SbO2 (mp-230) | 0.6515 | 0.000 | 2 |
SrLiEuTeO6 (mp-676932) | 0.7232 | 0.056 | 5 |
Ca14La6Mg3Ti17O60 (mp-695227) | 0.7290 | 0.011 | 5 |
NaLaMnWO6 (mp-25027) | 0.6907 | 0.114 | 5 |
LaZnFeCuO6 (mvc-9037) | 0.7284 | 0.292 | 5 |
CaLaCrNiO6 (mvc-9984) | 0.7215 | 0.075 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Sb O |
Final Energy/Atom-7.1091 eV |