material

ScCuSn

ID:

mp-13203

DOI:

10.17188/1189454


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.547 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgO (mp-1265) <1 1 1> <0 0 1> 0.000 219.7
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.003 276.1
GaSe (mp-1943) <1 0 1> <1 1 1> 0.004 276.1
GaSe (mp-1943) <0 0 1> <0 0 1> 0.013 50.7
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.015 212.4
Cu (mp-30) <1 1 1> <0 0 1> 0.020 67.6
GaAs (mp-2534) <1 0 0> <1 0 0> 0.022 364.2
Ge (mp-32) <1 0 0> <1 0 0> 0.028 364.2
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.029 202.8
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.029 321.1
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.030 364.2
PbSe (mp-2201) <1 1 1> <0 0 1> 0.030 67.6
CdSe (mp-2691) <1 0 0> <0 0 1> 0.033 270.4
GaSb (mp-1156) <1 0 0> <0 0 1> 0.034 270.4
ZrO2 (mp-2858) <0 1 0> <1 0 1> 0.037 138.9
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.038 67.6
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.039 67.6
CsI (mp-614603) <1 1 0> <1 0 1> 0.041 173.7
Mg (mp-153) <1 0 1> <0 0 1> 0.044 321.1
PbSe (mp-2201) <1 0 0> <0 0 1> 0.044 270.4
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.047 270.4
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.048 364.2
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.048 333.8
BN (mp-984) <1 0 0> <0 0 1> 0.050 135.2
LaF3 (mp-905) <0 0 1> <0 0 1> 0.052 321.1
GaSb (mp-1156) <1 1 1> <0 0 1> 0.058 67.6
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.058 333.8
CaF2 (mp-2741) <1 1 0> <1 0 1> 0.060 173.7
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.060 182.1
YVO4 (mp-19133) <1 0 1> <1 1 1> 0.063 276.1
SiC (mp-8062) <1 0 0> <0 0 1> 0.065 135.2
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.065 253.5
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.065 253.5
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.075 270.4
InSb (mp-20012) <1 0 0> <0 0 1> 0.078 354.9
CdSe (mp-2691) <1 1 1> <0 0 1> 0.086 67.6
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.090 270.4
CdTe (mp-406) <1 0 0> <0 0 1> 0.093 354.9
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.094 67.6
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.097 270.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.102 304.2
GaP (mp-2490) <1 1 0> <1 0 1> 0.104 173.7
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.108 273.1
InAs (mp-20305) <1 0 0> <0 0 1> 0.113 270.4
Mg (mp-153) <1 0 0> <1 0 0> 0.118 182.1
Fe2O3 (mp-24972) <1 1 0> <1 0 0> 0.120 121.4
Fe2O3 (mp-24972) <1 0 0> <1 1 0> 0.120 210.2
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.123 212.4
Fe2O3 (mp-24972) <1 0 1> <1 1 1> 0.124 220.8
InAs (mp-20305) <1 1 0> <0 0 1> 0.125 270.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
168 68 43 0 0 0
68 168 43 0 0 0
43 43 128 0 0 0
0 0 0 61 0 0
0 0 0 0 61 0
0 0 0 0 0 50
Compliance Tensor Sij (10-12Pa-1)
7.4 -2.6 -1.6 0 0 0
-2.6 7.4 -1.6 0 0 0
-1.6 -1.6 8.9 0 0 0
0 0 0 16.4 0 0
0 0 0 0 16.4 0
0 0 0 0 0 20
Shear Modulus GV
55 GPa
Bulk Modulus KV
86 GPa
Shear Modulus GR
54 GPa
Bulk Modulus KR
83 GPa
Shear Modulus GVRH
55 GPa
Bulk Modulus KVRH
84 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
DySnAu (mp-31414) 0.1234 0.000 3
HoSnAu (mp-568814) 0.1162 0.038 3
TmSnAu (mp-16741) 0.1108 0.048 3
LuCuPb (mp-16753) 0.1087 0.000 3
ErSnAu (mp-13303) 0.1027 0.043 3
EuTl2 (mp-30630) 0.5090 0.000 2
EuIn2 (mp-636316) 0.4810 0.000 2
YbIn2 (mp-568058) 0.4925 0.000 2
ThHg2 (mp-2215) 0.5262 0.000 2
CaIn2 (mp-21068) 0.5050 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Cu_pv Sn_d
Final Energy/Atom
-5.3546 eV
Corrected Energy
-32.1274 eV
Uncorrected energy = -32.1274 eV Corrected energy = -32.1274 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)