material

CaZn2

ID:

mp-13364

DOI:

10.17188/1189545


Tags: Calicum zinc (1/2) - HP

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.274 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.025 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.65 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CaZn2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 418878 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 1 1> <0 0 1> 0.001 359.1
C (mp-48) <0 0 1> <0 0 1> 0.001 110.5
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.002 193.4
AlN (mp-661) <0 0 1> <0 0 1> 0.003 110.5
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.006 349.3
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.011 331.5
Au (mp-81) <1 1 1> <0 0 1> 0.018 359.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.018 248.6
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.018 248.6
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.023 165.7
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.029 221.0
Fe2O3 (mp-24972) <1 1 1> <1 0 0> 0.031 249.5
C (mp-48) <1 0 0> <1 1 1> 0.035 272.2
TiO2 (mp-390) <1 1 1> <1 1 1> 0.038 272.2
Au (mp-81) <1 0 0> <1 0 1> 0.042 228.1
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.043 171.1
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.043 114.1
ZnO (mp-2133) <1 1 0> <1 0 0> 0.046 149.7
Mg (mp-153) <0 0 1> <0 0 1> 0.047 248.6
TiO2 (mp-390) <1 0 0> <0 0 1> 0.057 110.5
SiC (mp-8062) <1 0 0> <1 0 0> 0.058 349.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.070 303.9
Al (mp-134) <1 1 0> <1 0 1> 0.070 114.1
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.078 331.5
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.081 342.2
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.081 285.2
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.081 249.5
Ag (mp-124) <1 0 0> <1 0 1> 0.083 228.1
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.084 249.5
C (mp-66) <1 1 0> <1 0 1> 0.094 285.2
Ni (mp-23) <1 1 0> <0 0 1> 0.097 138.1
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.108 331.5
Te2W (mp-22693) <0 0 1> <1 0 0> 0.110 349.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.110 27.6
BN (mp-984) <0 0 1> <0 0 1> 0.113 193.4
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.114 221.0
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.115 285.2
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.122 359.1
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.123 193.4
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.124 349.3
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.127 27.6
ZnO (mp-2133) <1 0 0> <1 0 0> 0.133 349.3
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.136 221.0
TiO2 (mp-390) <1 1 0> <1 1 0> 0.137 259.3
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.139 349.3
Ni (mp-23) <1 0 0> <0 0 1> 0.140 193.4
GaSe (mp-1943) <1 0 0> <1 0 0> 0.142 199.6
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.144 172.8
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.154 342.2
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.157 331.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
85 29 26 0 0 0
29 85 26 0 0 0
26 26 97 0 0 0
0 0 0 26 0 0
0 0 0 0 26 0
0 0 0 0 0 28
Compliance Tensor Sij (10-12Pa-1)
14 -3.9 -2.7 0 0 0
-3.9 14 -2.7 0 0 0
-2.7 -2.7 11.8 0 0 0
0 0 0 38.4 0 0
0 0 0 0 38.4 0
0 0 0 0 0 35.7
Shear Modulus GV
28 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
28 GPa
Bulk Modulus KR
48 GPa
Shear Modulus GVRH
28 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca2Mg3Si (mp-1095343) 0.0672 0.119 3
Er2Al3Co (mp-567849) 0.1483 0.000 3
Nb2Co3Si (mp-10366) 0.1056 0.000 3
Lu2Al3Co (mp-16490) 0.1590 0.000 3
Mg2Cu3Si (mp-10746) 0.0651 0.000 3
ZrCr2 (mp-1919) 0.0985 0.020 2
CaCd2 (mp-1078) 0.0986 0.010 2
MgAg2 (mp-1094121) 0.1131 0.110 2
CdCu2 (mp-16775) 0.0875 0.017 2
YZn2 (mp-1095495) 0.0692 0.030 2
Co (mp-1072089) 0.2869 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Zn
Final Energy/Atom
-1.7827 eV
Corrected Energy
-21.3921 eV
Uncorrected energy = -21.3921 eV Corrected energy = -21.3921 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 418878
Submitted by
User remarks:
  • Calicum zinc (1/2) - HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)