Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.394 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 245.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 295.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 245.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.1 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 278.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 196.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 344.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 208.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 196.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 344.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 278.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 170.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 196.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 278.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 245.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 208.7 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 255.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 278.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 85.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 147.6 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 85.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 69.6 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 208.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 69.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 344.3 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 147.6 |
Al (mp-134) | <1 1 0> | <1 1 0> | 69.6 |
Al (mp-134) | <1 1 1> | <1 1 1> | 85.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 245.9 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 255.6 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 208.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 255.6 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 208.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 344.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 344.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 245.9 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 196.8 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 278.3 |
C (mp-66) | <1 0 0> | <1 1 1> | 255.6 |
C (mp-66) | <1 1 1> | <1 0 0> | 344.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 170.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 245.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 147.6 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 255.6 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 278.3 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 278.3 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 245.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 147.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 208.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
194 | 116 | 116 | 0 | 0 | 0 |
116 | 194 | 116 | 0 | 0 | 0 |
116 | 116 | 194 | 0 | 0 | 0 |
0 | 0 | 0 | 67 | 0 | 0 |
0 | 0 | 0 | 0 | 67 | 0 |
0 | 0 | 0 | 0 | 0 | 67 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.3 | -3.5 | -3.5 | 0 | 0 | 0 |
-3.5 | 9.3 | -3.5 | 0 | 0 | 0 |
-3.5 | -3.5 | 9.3 | 0 | 0 | 0 |
0 | 0 | 0 | 14.8 | 0 | 0 |
0 | 0 | 0 | 0 | 14.8 | 0 |
0 | 0 | 0 | 0 | 0 | 14.8 |
Shear Modulus GV56 GPa |
Bulk Modulus KV142 GPa |
Shear Modulus GR52 GPa |
Bulk Modulus KR142 GPa |
Shear Modulus GVRH54 GPa |
Bulk Modulus KVRH142 GPa |
Elastic Anisotropy0.37 |
Poisson's Ratio0.33 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeMnNi4 (mp-990536) | 0.0008 | 0.034 | 3 |
UZnNi4 (mp-21899) | 0.0008 | 0.000 | 3 |
UAlNi4 (mp-16519) | 0.0008 | 0.047 | 3 |
GdMgNi4 (mp-977381) | 0.0008 | 0.000 | 3 |
YMgCu4 (mp-13172) | 0.0021 | 0.000 | 3 |
DyCu5 (mp-30578) | 0.0008 | 0.004 | 2 |
HoCu5 (mp-580364) | 0.0027 | 0.007 | 2 |
ErCu5 (mp-30579) | 0.0053 | 0.000 | 2 |
TbCu5 (mp-1077262) | 0.0008 | 0.007 | 2 |
ZrNi5 (mp-905383) | 0.0041 | 0.001 | 2 |
Co (mp-1072089) | 0.0353 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ce Mg_pv Ni_pv |
Final Energy/Atom-5.5030 eV |
Corrected Energy-33.0180 eV
-33.0180 eV = -33.0180 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)