Final Magnetic Moment0.148 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.828 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSmSe + Sm2Se3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI43d [220] |
HallI 4bd 2c 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 135.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 78.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 110.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 78.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 110.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 78.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 110.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 156.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 221.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 135.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 235.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 313.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 313.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 313.4 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 221.6 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 235.0 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 135.7 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 313.4 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 235.0 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 110.8 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 313.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 156.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 313.4 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 313.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 156.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 78.3 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 110.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 221.6 |
Au (mp-81) | <1 0 0> | <1 0 0> | 156.7 |
Au (mp-81) | <1 1 0> | <1 1 0> | 221.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 78.3 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 156.7 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 235.0 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 78.3 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 110.8 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 156.7 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 235.0 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 235.0 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 110.8 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 156.7 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 135.7 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 313.4 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 313.4 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 110.8 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 78.3 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 156.7 |
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 221.6 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 78.3 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 156.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm(GdS2)2 (mp-676424) | 0.0415 | 0.027 | 3 |
Ce3AsS3 (mp-675514) | 0.0795 | 0.024 | 3 |
Ca(Ce2Se3)4 (mp-38870) | 0.0736 | 0.004 | 3 |
YbPr11Se16 (mp-531712) | 0.0846 | 0.016 | 3 |
Ce2SmS4 (mp-37045) | 0.0765 | 0.025 | 3 |
Gd3Se4 (mp-672292) | 0.0139 | 0.011 | 2 |
Np3Se4 (mp-570181) | 0.0155 | 0.035 | 2 |
Ce4Sb3 (mp-20680) | 0.0085 | 0.000 | 2 |
Tb4Bi3 (mp-570759) | 0.0104 | 0.031 | 2 |
Sm3S4 (mp-2038) | 0.0114 | 0.045 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Se |
Final Energy/Atom-5.8477 eV |
Corrected Energy-81.8676 eV
-81.8676 eV = -81.8676 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)